ABSTRACT:
Disclosed are methods of forming dielectric materials using atomic layer deposition (ALD) and methods of forming dielectric layers from such materials on a semiconductor device. The ALD process utilizes a first reactant containing at least one alkoxide group that is chemisorbed onto a surface of a substrate and then reacted with an activated oxidant that contains no hydroxyl group to form a dielectric material exhibiting excellent step coverage and improved leakage current characteristics.

REFERENCES:
patent: 6632279 (2003-10-01), Ritala et al.
patent: 6664186 (2003-12-01), Callegari et al.
patent: 6743475 (2004-06-01), Skarp et al.
patent: 6780704 (2004-08-01), Raajimakers et al.
patent: 7007933 (2006-03-01), Lee et al.
patent: 2003/0040196 (2003-02-01), Lim et al.
patent: 2003/0113480 (2003-06-01), Kil et al.
patent: 2004/0009307 (2004-01-01), Koh et al.
patent: 2004/0065253 (2004-04-01), Tois et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of forming material using atomic layer deposition and... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of forming material using atomic layer deposition and..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of forming material using atomic layer deposition and... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3952219

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.