Semiconductor device manufacturing: process – Making field effect device having pair of active regions... – Having insulated gate
Reexamination Certificate
2008-07-01
2008-07-01
Nhu, David (Department: 2818)
Semiconductor device manufacturing: process
Making field effect device having pair of active regions...
Having insulated gate
C438S381000, C438S680000, C438S778000, C257SE21170, C257SE21126, C257SE21127, C257SE21278, C257SE21293, C257SE21632, C257SE21645
Reexamination Certificate
active
07393736
ABSTRACT:
The use of atomic layer deposition (ALD) to form a nanolaminate dielectric of zirconium oxide (ZrO2), hafnium oxide (HfO2) and tin oxide (SnO2) acting as a single dielectric layer with a formula of ZrXHfYSn1-X-YO2, and a method of fabricating such a dielectric layer is described that produces a reliable structure with a high dielectric constant (high k). The dielectric structure is formed by depositing zirconium oxide by atomic layer deposition onto a substrate surface using precursor chemicals, followed by depositing hafnium oxide onto the substrate using precursor chemicals, followed by depositing tin oxide onto the substrate using precursor chemicals, and repeating to form the thin laminate structure. Such a dielectric may be used as a gate insulator, a capacitor dielectric, or as a tunnel insulator in non-volatile memories, because the high dielectric constant (high k) provides the functionality of a much thinner silicon dioxide film.
REFERENCES:
patent: 5912797 (1999-06-01), Schneemeyer et al.
patent: 6200893 (2001-03-01), Sneh
patent: 6451695 (2002-09-01), Sneh
patent: 6495436 (2002-12-01), Ahn et al.
patent: 6514828 (2003-02-01), Ahn et al.
patent: 6534420 (2003-03-01), Ahn et al.
patent: 6537613 (2003-03-01), Senzaki et al.
patent: 6608378 (2003-08-01), Ahn et al.
patent: 6661058 (2003-12-01), Ahn et al.
patent: 6767795 (2004-07-01), Ahn et al.
patent: 6787413 (2004-09-01), Ahn
patent: 6844203 (2005-01-01), Ahn et al.
patent: 6893984 (2005-05-01), Ahn et al.
patent: 6900122 (2005-05-01), Ahn et al.
patent: 6921702 (2005-07-01), Ahn et al.
patent: 6953730 (2005-10-01), Ahn et al.
patent: 6958302 (2005-10-01), Ahn et al.
patent: 6960538 (2005-11-01), Ahn et al.
patent: 6967154 (2005-11-01), Meng et al.
patent: 7026694 (2006-04-01), Ahn et al.
patent: 7045205 (2006-05-01), Sager
patent: 7101813 (2006-09-01), Ahn et al.
patent: 7169673 (2007-01-01), Ahn et al.
patent: 7205218 (2007-04-01), Ahn et al.
patent: 2002/0024080 (2002-02-01), Derderian et al.
patent: 2002/0024108 (2002-02-01), Lucovsky et al.
patent: 2002/0025628 (2002-02-01), Derderian et al.
patent: 2002/0046705 (2002-04-01), Sandhu et al.
patent: 2002/0192974 (2002-12-01), Anh et al.
patent: 2002/0192975 (2002-12-01), Ahn
patent: 2003/0043637 (2003-03-01), Forbes et al.
patent: 2003/0045078 (2003-03-01), Ahn et al.
patent: 2003/0045082 (2003-03-01), Eldridge et al.
patent: 2003/0048666 (2003-03-01), Eldridge et al.
patent: 2003/0175411 (2003-09-01), Kodas et al.
patent: 2003/0207032 (2003-11-01), Ahn et al.
patent: 2003/0207540 (2003-11-01), Ahn et al.
patent: 2003/0207593 (2003-11-01), Derderian
patent: 2003/0227033 (2003-12-01), Ahn et al.
patent: 2003/0228747 (2003-12-01), Ahn et al.
patent: 2004/0043541 (2004-03-01), Ahn
patent: 2004/0043569 (2004-03-01), Ahn
patent: 2004/0065255 (2004-04-01), Yang et al.
patent: 2004/0110391 (2004-06-01), Ahn et al.
patent: 2004/0144980 (2004-07-01), Ahn et al.
patent: 2004/0164357 (2004-08-01), Ahn et al.
patent: 2004/0175882 (2004-09-01), Ahn et al.
patent: 2004/0183108 (2004-09-01), Ahn
patent: 2004/0185654 (2004-09-01), Ahn
patent: 2004/0214399 (2004-10-01), Ahn et al.
patent: 2004/0222476 (2004-11-01), Ahn et al.
patent: 2004/0262700 (2004-12-01), Ahn et al.
patent: 2005/0009370 (2005-01-01), Ahn
patent: 2005/0020017 (2005-01-01), Ahn et al.
patent: 2005/0023594 (2005-02-01), Ahn et al.
patent: 2005/0023624 (2005-02-01), Ahn et al.
patent: 2005/0023625 (2005-02-01), Ahn et al.
patent: 2005/0023626 (2005-02-01), Ahn et al.
patent: 2005/0026349 (2005-02-01), Forbes et al.
patent: 2005/0029547 (2005-02-01), Ahn et al.
patent: 2005/0029604 (2005-02-01), Ahn et al.
patent: 2005/0029605 (2005-02-01), Ahn et al.
patent: 2005/0032292 (2005-02-01), Ahn et al.
patent: 2005/0037563 (2005-02-01), Ahn
patent: 2005/0054165 (2005-03-01), Ahn et al.
patent: 2005/0077519 (2005-04-01), Ahn et al.
patent: 2005/0124175 (2005-06-01), Ahn et al.
patent: 2005/0158973 (2005-07-01), Ahn et al.
patent: 2005/0164521 (2005-07-01), Ahn et al.
patent: 2005/0215015 (2005-09-01), Ahn et al.
patent: 2005/0218462 (2005-10-01), Ahn et al.
patent: 2005/0227442 (2005-10-01), Ahn et al.
patent: 03028162 (1991-02-01), None
patent: WO-02/31875 (2002-04-01), None
patent: WO-02/43115 (2002-05-01), None
Ahn, Kie Y., et al., “Ald of Amorphous Lanthanide Doped Tiox Films”, U.S. Appl. No. 11/092,072; filed Mar. 29, 2005.
Ahn, Kie Y., et al., “Atomic Layer Deposited Hafnium Tantalum Oxide Dielectrics”, U.S. Appl. No. 11/029,757; filed Jan. 5, 2005.
Ahn, Kie Y., et al., “Atomic Layer Deposited Lanthanum Aluminum Oxide Dielectric Layer”, U.S. Appl. No. 10/930,167; filed Aug. 31, 2004.
Ahn, Kie Y., et al., “Atomic Layer Deposited Lanthanum Hafnium Oxide Dielectrics”, U.S. Appl. No. 11/010,529; filed Dec. 13, 2004.
Ahn, Kie Y., et al., “Atomic Layer Deposited Titanium Aluminum Oxide Films”, U.S. Appl. No. 10/931,533; filed Aug. 31, 2004.
Ahn, Kie Y., et al., “Atomic Layer Deposited Titanium Silicon Oxide Films”, U.S. Appl. No. 11/093,104; filed Mar. 29, 2005.
Ahn, Kie Y., et al., “Atomic Layer Deposited Zirconium Silicon Oxide Films”, U.S. Appl. No. 11/117,121; filed Apr. 28, 2005.
Ahn, Kie Y., et al., “Atomic Layer Deposition of a Ruthenium Layer to a Lanthanide Oxide Dielectric Layer”, U.S. Appl. No. 11/117,125; filed Apr. 28, 2005.
Ahn, Kie Y., et al., “Atomic Layer Deposition of CEO/AL2O3 Films as Gate Dielectrics”, U.S. Appl. No. 11/055,380; filed Feb. 10, 2005.
Ahn, Kie Y., et al., “Atomic Layer Deposition of DY-Doped HFO2 Films as Gate Dielectrics”, U.S. Appl. No. 11/053,577; filed Feb. 8, 2005.
Ahn, Kie Y., et al., “Atomic Layer Deposition of Zirconium-Doped Tantalum Oxide Films”, U.S. Appl. No. 10/909,959; filed Aug. 2, 2004.
Ahn, Kie Y., et al., “Hafnium Titanium Oxide Films”, U.S. Appl. No. 11/140,643, filed May 27, 2005.
Ahn, Kie Y., et al., “Hybrid ALD-CVD of PrXOY/ZrO2 Films as Gate Dielectrics”, U.S. Appl. No. 11/010,766; filed Dec. 13, 2004.
Ahn, Kie Y., et al., “Iridium / Zirconium Oxide Structure”, U.S. Appl. No. 11/152,759; filed Jun. 14, 2005.
Ahn, Kie Y., et al., “Ruthenium Gate for a Lanthanide Oxide Dielectric Layer”, U.S. Appl. No. 10/926,812; filed Aug. 26, 2004.
Ahn, Kie Y., et al., “Semiconductor Constructions Comprising Cerium Oxide and Titanium Oxide; and Methods of Forming Semiconductor Constructions”, U.S. Appl. No. 10/881,874, filed Jun. 29, 2004.
Non-final office action mailed May 22, 2007 in Serial No. 11-216474, 20 pgs.
Aarik, Jaan , et al., “Influence of substrate temperature on atomic layer growth and properties of HfO/sub 2/ thin films”,Thin Solid Films, 340(1-2), (1999), 110-116.
Aarik, Jaan , et al., “Phase transformations in hafnium dioxide thin films grown by atomic layer deposition at high temperatures”,Applied Surface Science, 173(1-2), (Mar. 2001), 15-21.
Aarik, Jaan , et al., “Texture development in nanocrystalline hafnium dioxide thin films grown by atomic layer deposition”,Journal of Crystal Growth, 220(1-2), (Nov. 15, 2000), 105-113.
Conley, J. F., et al., “Atomic Layer Deposition of Hafnium Oxide Using Anhydrous Hafnium Nitrate”,Electrochemical and Solid-State Letters, 5(5), (May 2002), C57-C59.
Endo, Kazuhiko , et al., “Metal Organic Atomic Layer Deposition of High-k Gate Dielectrics Using Plasma Oxidation”,Japanese Journal of Applied Physics, 42, (2003), L685-L687.
Hubbard, K. J., et al., “Thermodynamic stability of binary oxides in contact with silicon”,Journal of Materials Research, 11(11), (Nov. 1996), 2757-2776.
Ishii, Hiroyuki, et al., “Growth and electrical properties of atomic-layer deposited ZrO2/Si-nitride stack gate dielectrics”,Journal of Applied Physics, 95(2), (Jan. 15, 2004), 536-542.
Jonsson, A. K., et al., “Dielectric Permittivity and Intercalation Parameters of Li Ion Intercalated Atomic Layer Deposited ZrO2”,Journal of
Ahn Kie Y.
Forbes Leonard
Micro)n Technology, Inc.
Nhu David
Schwegman Lundberg & Woessner, P.A.
LandOfFree
Atomic layer deposition of Zr x Hf y Sn 1-x-y O 2 films... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Atomic layer deposition of Zr x Hf y Sn 1-x-y O 2 films..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Atomic layer deposition of Zr x Hf y Sn 1-x-y O 2 films... will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2742915