Semiconductor device manufacturing: process – Coating of substrate containing semiconductor region or of...
Reexamination Certificate
2008-01-01
2008-01-01
Smith, Bradley K (Department: 2891)
Semiconductor device manufacturing: process
Coating of substrate containing semiconductor region or of...
C257SE21161
Reexamination Certificate
active
07314835
ABSTRACT:
A method for depositing a film on a substrate using a plasma enhanced atomic layer deposition (PEALD) process includes disposing the substrate in a process chamber configured to facilitate the PEALD process. A first process material is introduced within the process chamber, and a second process material is introduced within the process chamber. Electromagnetic power of more than 600 W is coupled to the process chamber during introduction of the second process material in order to generate a plasma that accelerates a reduction reaction between the first and second process materials at a surface of the substrate. The film is formed on the substrate by alternatingly introducing the first process material and the second process material.
REFERENCES:
patent: 2004/0151844 (2004-08-01), Zhang et al.
patent: 2006/0177579 (2006-08-01), Shin et al.
Ishizaka Tadahiro
Yamamoto Kaoru
Oblon & Spivak, McClelland, Maier & Neustadt P.C.
Smith Bradley K
Tokyo Electron Limited
LandOfFree
Plasma enhanced atomic layer deposition system and method does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Plasma enhanced atomic layer deposition system and method, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Plasma enhanced atomic layer deposition system and method will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2795228