Gas delivery apparatus and method for atomic layer deposition

Adhesive bonding and miscellaneous chemical manufacture – Differential fluid etching apparatus – With gas inlet structure

Reexamination Certificate

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C156S345420, C156S039000, C118S715000

Reexamination Certificate

active

06916398

ABSTRACT:
One embodiment of the gas delivery assembly comprises a covering member having an expanding channel at a central portion of the covering member and having a bottom surface extending from the expanding channel to a peripheral portion of the covering member. One or more gas conduits are coupled to the expanding channel in which the one or more gas conduits are positioned at an angle from a center of the expanding channel. One embodiment of a chamber comprises a substrate support having a substrate receiving surface. The chamber further includes a chamber lid having a passageway at a central portion of the chamber lid and a tapered bottom surface extending from the passageway to a peripheral portion of the chamber lid. The bottom surface of the chamber lid is shaped and sized to substantially cover the substrate receiving surface. One or more valves are coupled to the passageway, and one or more gas sources are coupled to each valve. In one aspect, the bottom surface of the chamber lid may be tapered. In another aspect, a reaction zone defined between the chamber lid and the substrate receiving surface may comprise a small volume. In still another aspect, the passageway may comprise a tapered expanding channel extending from the central portion of the chamber lid. Another embodiment of the chamber comprises a substrate support having a substrate receiving surface. The chamber further comprises a chamber lid having an expanding channel extending from a central portion of the chamber lid and having a tapered bottom surface extending from the expanding channel to a peripheral portion of the chamber lid. One or more gas conduits are disposed around an upper portion of the expanding channel in which the one or more gas conduits are disposed at an angle from a center of the expanding channel. A choke is disposed on the chamber lid adjacent a perimeter of the tapered bottom surface.

REFERENCES:
patent: 3291456 (1966-12-01), Deane
patent: 4058430 (1977-11-01), Suntola et al.
patent: 4389973 (1983-06-01), Suntola et al.
patent: 4413022 (1983-11-01), Suntola et al.
patent: 4486487 (1984-12-01), Skarp
patent: 4614639 (1986-09-01), Hegedus
patent: 4732110 (1988-03-01), Parsons
patent: 4761269 (1988-08-01), Conger et al.
patent: 4767494 (1988-08-01), Kobayashi et al.
patent: 4806321 (1989-02-01), Nishizawa et al.
patent: 4813846 (1989-03-01), Helms
patent: 4829022 (1989-05-01), Kobayashi et al.
patent: 4834831 (1989-05-01), Nishizawa et al.
patent: 4838983 (1989-06-01), Schumaker et al.
patent: 4838993 (1989-06-01), Aoki et al.
patent: 4840921 (1989-06-01), Matsumoto
patent: 4845049 (1989-07-01), Sunakawa
patent: 4859625 (1989-08-01), Matsumoto
patent: 4859627 (1989-08-01), Sunakawa
patent: 4861417 (1989-08-01), Mochizuki et al.
patent: 4876218 (1989-10-01), Pessa et al.
patent: 4907534 (1990-03-01), Huang et al.
patent: 4917556 (1990-04-01), Stark et al.
patent: 4927670 (1990-05-01), Erbil
patent: 4931132 (1990-06-01), Aspnes et al.
patent: 4951601 (1990-08-01), Maydan et al.
patent: 4960720 (1990-10-01), Shimbo
patent: 4975252 (1990-12-01), Nishizawa et al.
patent: 4987856 (1991-01-01), Hey et al.
patent: 4991542 (1991-02-01), Kohmura et al.
patent: 4993357 (1991-02-01), Scholz
patent: 5000113 (1991-03-01), Wang et al.
patent: 5013683 (1991-05-01), Petroff et al.
patent: 5028565 (1991-07-01), Chang et al.
patent: 5082798 (1992-01-01), Arimoto
patent: 5085885 (1992-02-01), Foley et al.
patent: 5085887 (1992-02-01), Adams et al.
patent: 5091320 (1992-02-01), Aspnes et al.
patent: 5130269 (1992-07-01), Kitahara et al.
patent: 5134965 (1992-08-01), Tokuda et al.
patent: 5166092 (1992-11-01), Mochizuki et al.
patent: 5173474 (1992-12-01), Connell et al.
patent: 5186718 (1993-02-01), Tepman et al.
patent: 5204145 (1993-04-01), Gasworth
patent: 5205077 (1993-04-01), Wittstock
patent: 5221449 (1993-06-01), Colgan et al.
patent: 5224513 (1993-07-01), Bertone
patent: 5225366 (1993-07-01), Yoder
patent: 5234561 (1993-08-01), Randhawa et al.
patent: 5246536 (1993-09-01), Nishizawa et al.
patent: 5250148 (1993-10-01), Nishizawa et al.
patent: 5254207 (1993-10-01), Nishizawa et al.
patent: 5256244 (1993-10-01), Ackerman
patent: 5259881 (1993-11-01), Edwards et al.
patent: 5261959 (1993-11-01), Gasworth
patent: 5264038 (1993-11-01), Hara et al.
patent: 5270247 (1993-12-01), Sakuma et al.
patent: 5278435 (1994-01-01), Van Hove et al.
patent: 5281274 (1994-01-01), Yoder
patent: 5281485 (1994-01-01), Colgan et al.
patent: 5286296 (1994-02-01), Sato et al.
patent: 5290748 (1994-03-01), Knuuttila et al.
patent: 5294286 (1994-03-01), Nishizawa et al.
patent: 5296403 (1994-03-01), Nishizawa et al.
patent: 5300186 (1994-04-01), Kitahara et al.
patent: 5306666 (1994-04-01), Izumi
patent: 5311055 (1994-05-01), Goodman et al.
patent: 5316615 (1994-05-01), Copel
patent: 5316793 (1994-05-01), Wallace et al.
patent: 5330610 (1994-07-01), Eres et al.
patent: 5336324 (1994-08-01), Stall et al.
patent: 5338362 (1994-08-01), Imahashi
patent: 5338363 (1994-08-01), Kawata et al.
patent: 5338364 (1994-08-01), Kurihara et al.
patent: 5338389 (1994-08-01), Nishizawa et al.
patent: 5348911 (1994-09-01), Jurgensen et al.
patent: 5374570 (1994-12-01), Nasu et al.
patent: 5395791 (1995-03-01), Cheng et al.
patent: 5438952 (1995-08-01), Otsuka
patent: 5439876 (1995-08-01), Graf et al.
patent: 5441703 (1995-08-01), Jurgensen
patent: 5443033 (1995-08-01), Nishizawa et al.
patent: 5443647 (1995-08-01), Aucoin et al.
patent: 5455072 (1995-10-01), Bension et al.
patent: 5458084 (1995-10-01), Thorne et al.
patent: 5469806 (1995-11-01), Mochizuki et al.
patent: 5480818 (1996-01-01), Matsumoto et al.
patent: 5483919 (1996-01-01), Yokoyama et al.
patent: 5484664 (1996-01-01), Kitahara et al.
patent: 5496410 (1996-03-01), Fukuda et al.
patent: 5503875 (1996-04-01), Imai et al.
patent: 5521126 (1996-05-01), Okamura et al.
patent: 5527733 (1996-06-01), Nishizawa et al.
patent: 5532511 (1996-07-01), Nishizawa et al.
patent: 5540783 (1996-07-01), Eres et al.
patent: 5542452 (1996-08-01), Carver et al.
patent: 5573566 (1996-11-01), Anderberg et al.
patent: 5580380 (1996-12-01), Liu et al.
patent: 5601651 (1997-02-01), Watabe
patent: 5609689 (1997-03-01), Kato et al.
patent: 5616181 (1997-04-01), Yamamoto et al.
patent: 5637530 (1997-06-01), Gaines et al.
patent: 5641984 (1997-06-01), Aftergut et al.
patent: 5643366 (1997-07-01), Somekh et al.
patent: 5644128 (1997-07-01), Wollnik et al.
patent: 5667592 (1997-09-01), Boitnott et al.
patent: 5674786 (1997-10-01), Turner et al.
patent: 5693139 (1997-12-01), Nishizawa et al.
patent: 5695564 (1997-12-01), Imahashi
patent: 5705224 (1998-01-01), Murota et al.
patent: 5707880 (1998-01-01), Aftergut et al.
patent: 5711811 (1998-01-01), Suntola et al.
patent: 5730801 (1998-03-01), Tepman et al.
patent: 5730802 (1998-03-01), Ishizumi et al.
patent: 5747113 (1998-05-01), Tsai
patent: 5749974 (1998-05-01), Habuka et al.
patent: 5788447 (1998-08-01), Yonemitsu et al.
patent: 5788799 (1998-08-01), Steger et al.
patent: 5796116 (1998-08-01), Nakata et al.
patent: 5801634 (1998-09-01), Young et al.
patent: 5804488 (1998-09-01), Shih et al.
patent: 5807792 (1998-09-01), Ilg et al.
patent: 5830270 (1998-11-01), McKee et al.
patent: 5835677 (1998-11-01), Li et al.
patent: 5838677 (1998-11-01), Kozaki et al.
patent: 5846330 (1998-12-01), Quirk et al.
patent: 5851849 (1998-12-01), Comizzoli et al.
patent: 5855675 (1999-01-01), Doering et al.
patent: 5855680 (1999-01-01), Soininen et al.
patent: 5856219 (1999-01-01), Naito et al.
patent: 5858102 (1999-01-01), Tsai
patent: 5866213 (1999-02-01), Foster et al.
patent: 5866795 (1999-02-01), Wang et al.
patent: 5879459 (1999-03-01), Gadgil et al.
patent: 5882165 (1999-03-01), Maydan et al.
patent: 5882413 (1999-03-01), Beaulieu et al.
patent: 5888303 (1999-03-01), Dixon
patent: 5904565 (1999-05-01), Nguyen et al.
patent: 5916365 (1999-06-01), Sherman
patent: 5919332 (1999-07-01), Koshiishi et al.
patent: 5923056 (1999-07-01), Lee et al.
patent: 5923985 (1999-07-01), Aoki et al.
patent: 5925574 (1999-07-01), Aoki et al.
patent: 5928389 (1999-07-01), Jevtic
patent: 5942040 (1

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Gas delivery apparatus and method for atomic layer deposition does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Gas delivery apparatus and method for atomic layer deposition, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Gas delivery apparatus and method for atomic layer deposition will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3380468

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.