ABSTRACT:
The use of atomic layer deposition (ALD) to form a dielectric layer of zirconium nitride (Zr3N4) and zirconium oxide (ZrO2) and a method of fabricating such a dielectric layer produces a reliable structure for use in a variety of electronic devices. Forming the dielectric structure includes depositing zirconium oxide using atomic layer deposition using precursor chemicals, followed by depositing zirconium nitride using precursor chemicals, and repeating. Alternatively, the zirconium nitride may be deposited first followed by the zirconium nitride, thus providing a different work function. Such a dielectric may be used as the gate insulator of a MOSFET, a capacitor dielectric, or a tunnel gate insulator in memories, because the high dielectric constant (high-k) of the film provides the functionality of a thinner silicon dioxide film, and because of the reduced leakage current of the physically thicker dielectric layer when compared to an electrically equivalent thickness of silicon dioxide.

REFERENCES:
patent: 5572052 (1996-11-01), Kashihara et al.
patent: 5698022 (1997-12-01), Glassman et al.
patent: 6013553 (2000-01-01), Wallace et al.
patent: 6020024 (2000-02-01), Maiti et al.
patent: 6020243 (2000-02-01), Wallace et al.
patent: 6146976 (2000-11-01), Stecher et al.
patent: 6203613 (2001-03-01), Gates et al.
patent: 6297539 (2001-10-01), Ma et al.
patent: 6404027 (2002-06-01), Hong et al.
patent: 6436799 (2002-08-01), Ramkumar et al.
patent: 6444592 (2002-09-01), Ballantine et al.
patent: 6451695 (2002-09-01), Sneh
patent: 6495436 (2002-12-01), Ahn et al.
patent: 6514828 (2003-02-01), Ahn et al.
patent: 6534420 (2003-03-01), Ahn et al.
patent: 6559007 (2003-05-01), Weimer
patent: 6559014 (2003-05-01), Jeon
patent: 6608378 (2003-08-01), Forbes et al.
patent: 6617639 (2003-09-01), Wang et al.
patent: 6632279 (2003-10-01), Ritala et al.
patent: 6661058 (2003-12-01), Ahn et al.
patent: 6674138 (2004-01-01), Halliyal et al.
patent: 6699747 (2004-03-01), Ruff et al.
patent: 6710383 (2004-03-01), Yugami et al.
patent: 6737309 (2004-05-01), Matsuo
patent: 6767582 (2004-07-01), Elers
patent: 6767795 (2004-07-01), Ahn et al.
patent: 6770923 (2004-08-01), Nguyen et al.
patent: 6780704 (2004-08-01), Raaijmakers et al.
patent: 6787413 (2004-09-01), Ahn et al.
patent: 6790791 (2004-09-01), Ahn et al.
patent: 6821873 (2004-11-01), Visokay et al.
patent: 6831315 (2004-12-01), Raaijmakers et al.
patent: 6844203 (2005-01-01), Ahn et al.
patent: 6852645 (2005-02-01), Colombo et al.
patent: 6884739 (2005-04-01), Ahn et al.
patent: 6893984 (2005-05-01), Ahn et al.
patent: 6900122 (2005-05-01), Ahn et al.
patent: 6921702 (2005-07-01), Ahn et al.
patent: 6958302 (2005-10-01), Ahn et al.
patent: 6960538 (2005-11-01), Ahn et al.
patent: 6964893 (2005-11-01), Matsuo
patent: 6979855 (2005-12-01), Ahn et al.
patent: 6989565 (2006-01-01), Aronowitz et al.
patent: 6989573 (2006-01-01), Ahn et al.
patent: 7064048 (2006-06-01), Lai et al.
patent: 7067439 (2006-06-01), Metzner et al.
patent: 7071066 (2006-07-01), Wang et al.
patent: 7081421 (2006-07-01), Ahn et al.
patent: 7205620 (2007-04-01), Ahn et al.
patent: 2001/0030352 (2001-10-01), Ruf et al.
patent: 2002/0001971 (2002-01-01), Cho
patent: 2002/0037615 (2002-03-01), Matsuo
patent: 2002/0089023 (2002-07-01), Yu et al.
patent: 2002/0111001 (2002-08-01), Ahn
patent: 2002/0146916 (2002-10-01), Irino et al.
patent: 2002/0155688 (2002-10-01), Ahn
patent: 2002/0155689 (2002-10-01), Ahn
patent: 2002/0172768 (2002-11-01), Endo et al.
patent: 2002/0192974 (2002-12-01), Ahn et al.
patent: 2002/0192975 (2002-12-01), Ahn
patent: 2002/0192979 (2002-12-01), Ahn
patent: 2003/0003635 (2003-01-01), Paranipe et al.
patent: 2003/0003702 (2003-01-01), Ahn
patent: 2003/0017717 (2003-01-01), Ahn
patent: 2003/0043637 (2003-03-01), Forbes et al.
patent: 2003/0045078 (2003-03-01), Ahn et al.
patent: 2003/0048666 (2003-03-01), Eldrige et al.
patent: 2003/0059535 (2003-03-01), Luo et al.
patent: 2003/0116804 (2003-06-01), Visokay et al.
patent: 2003/0119246 (2003-06-01), Ahn
patent: 2003/0119291 (2003-06-01), Ahn et al.
patent: 2003/0132491 (2003-07-01), Ahn
patent: 2003/0139039 (2003-07-01), Ahn et al.
patent: 2003/0141560 (2003-07-01), Sun
patent: 2003/0157764 (2003-08-01), Ahn et al.
patent: 2003/0185980 (2003-10-01), Endo
patent: 2003/0207032 (2003-11-01), Ahn et al.
patent: 2003/0207540 (2003-11-01), Ahn et al.
patent: 2003/0227033 (2003-12-01), Ahn et al.
patent: 2003/0228747 (2003-12-01), Ahn et al.
patent: 2003/0232501 (2003-12-01), Kher et al.
patent: 2003/0232511 (2003-12-01), Metzner et al.
patent: 2004/0007171 (2004-01-01), Ritala et al.
patent: 2004/0023461 (2004-02-01), Ahn et al.
patent: 2004/0023516 (2004-02-01), Londergan et al.
patent: 2004/0038554 (2004-02-01), Ahn
patent: 2004/0043541 (2004-03-01), Ahn et al.
patent: 2004/0043569 (2004-03-01), Ahn et al.
patent: 2004/0110348 (2004-06-01), Ahn et al.
patent: 2004/0110391 (2004-06-01), Ahn et al.
patent: 2004/0144980 (2004-07-01), Ahn et al.
patent: 2004/0164357 (2004-08-01), Ahn et al.
patent: 2004/0175882 (2004-09-01), Ahn et al.
patent: 2004/0183108 (2004-09-01), Ahn
patent: 2004/0183143 (2004-09-01), Matsuo
patent: 2004/0185654 (2004-09-01), Ahn
patent: 2004/0198069 (2004-10-01), Metzner et al.
patent: 2004/0214399 (2004-10-01), Ahn et al.
patent: 2004/0222476 (2004-11-01), Ahn et al.
patent: 2004/0262700 (2004-12-01), Ahn et al.
patent: 2005/0009370 (2005-01-01), Ahn
patent: 2005/0020017 (2005-01-01), Ahn et al.
patent: 2005/0023594 (2005-02-01), Ahn et al.
patent: 2005/0023624 (2005-02-01), Ahn et al.
patent: 2005/0023625 (2005-02-01), Ahn et al.
patent: 2005/0023626 (2005-02-01), Ahn et al.
patent: 2005/0026349 (2005-02-01), Forbes et al.
patent: 2005/0029547 (2005-02-01), Ahn et al.
patent: 2005/0029604 (2005-02-01), Ahn et al.
patent: 2005/0029605 (2005-02-01), Ahn et al.
patent: 2005/0032292 (2005-02-01), Ahn et al.
patent: 2005/0037563 (2005-02-01), Ahn
patent: 2005/0054165 (2005-03-01), Ahn et al.
patent: 2005/0077519 (2005-04-01), Ahn et al.
patent: 2005/0227442 (2005-10-01), Ahn et al.
patent: 2005/0275033 (2005-12-01), Zhu et al.
patent: 2005/0277256 (2005-12-01), Ahn et al.
patent: 2005/0280067 (2005-12-01), Ahn et al.
patent: 2006/0003517 (2006-01-01), Ahn et al.
patent: 2006/0022283 (2006-02-01), Thomas et al.
patent: 2006/0024975 (2006-02-01), Ahn et al.
patent: 2006/0043492 (2006-03-01), Ahn et al.
patent: 2006/0043504 (2006-03-01), Ahn et al.
patent: 2006/0046522 (2006-03-01), Ahn et al.
patent: 2006/0054943 (2006-03-01), Li et al.
patent: 2006/0125030 (2006-06-01), Ahn et al.
patent: 2006/0128168 (2006-06-01), Ahn et al.
patent: 2006/0148180 (2006-07-01), Ahn et al.
patent: 2006/0189154 (2006-08-01), Ahn et al.
patent: 2006/0189164 (2006-08-01), Okabe et al.
patent: 2006/0208215 (2006-09-01), Metzner et al.
patent: 2006/0228868 (2006-10-01), Ahn et al.
patent: 2006/0246741 (2006-11-01), Ahn et al.
patent: 2006/0281330 (2006-12-01), Ahn et al.
patent: 2007/0007560 (2007-01-01), Forbes et al.
patent: 2007/0007635 (2007-01-01), Forbes et al.
patent: 2007/0010060 (2007-01-01), Forbes et al.
patent: 2007/0010061 (2007-01-01), Forbes et al.
patent: 2007/0045752 (2007-03-01), Forbes et al.
patent: 2007/0090440 (2007-04-01), Ahn et al.
patent: 0540993 (1993-05-01), None
patent: 1096042 (2001-05-01), None
patent: 1124262 (2001-08-01), None
Becker, Jill S., “Atomic Layer Deposition of Insulating Hafnium and Zirconium Nitrides”,Chem. Mater. 16, (2004), 3497-3501.
Bradley, D. C., “Metallo-organic Compounds Containing Metal-Nitrogen onds”,J. Chem Soc.(A), (1969), 980-984.
Bradley, D. C., “Metallo-organic Compounds containing metal-Nitrogen bonds”,J. Chem. Soc., (1960),3857-3861.
Copel, M., et al., “Strucutre and stability of ultrathin zirconium oxide layers on Si(001)”,Applied Physics Letters, 76(4), (Jan. 2000),436-438.
Iwamoto, K., “Advanced Layer-By-Layer Deposition and Annealing Process For High-Quality High-K Dielectrics Formation”,Electrochemical Society Proceedings vol. 2003(14), (2003),265-272.
Ko, Myoung-Gyun, et al.,

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Atomic layer deposition of Zr 3 N 4 /ZrO 2 films as gate... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Atomic layer deposition of Zr 3 N 4 /ZrO 2 films as gate..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Atomic layer deposition of Zr 3 N 4 /ZrO 2 films as gate... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3969186

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.