ABSTRACT:
The invention includes an atomic layer deposition method of forming a layer of a deposited composition on a substrate. The method includes positioning a semiconductor substrate within an atomic layer deposition chamber. On the substrate, an intermediate composition monolayer is formed, followed by a desired deposited composition from reaction with the intermediate composition, collectively from flowing multiple different composition deposition precursors to the substrate within the deposition chamber. A material adheres to a chamber internal component surface from such sequentially forming. After such sequentially forming, a reactive gas flows to the chamber which is different in composition from the multiple different deposition precursors and which is effective to react with such adhering material. After the reactive gas flowing, such sequentially forming is repeated. Further implementations are contemplated.

REFERENCES:
patent: 5225032 (1993-07-01), Golecki
patent: 5879459 (1999-03-01), Gadgil et al.
patent: 5925411 (1999-07-01), van de Ven et al.
patent: 5972430 (1999-10-01), DiMeo, Jr. et al.
patent: 6015597 (2000-01-01), David
patent: 6174377 (2001-01-01), Doering et al.
patent: 6197120 (2001-03-01), David
patent: 6200893 (2001-03-01), Sneh
patent: 6270572 (2001-08-01), Kim et al.
patent: 6287965 (2001-09-01), Kang et al.
patent: 6301434 (2001-10-01), McDiarmid et al.
patent: 6305314 (2001-10-01), Sneh et al.
patent: 6355561 (2002-03-01), Sandhu et al.
patent: 6387185 (2002-05-01), Doering et al.
patent: 6391785 (2002-05-01), Satta et al.
patent: 6403156 (2002-06-01), Jang et al.
patent: 6426307 (2002-07-01), Lim
patent: 6451119 (2002-09-01), Sneh et al.
patent: 6451695 (2002-09-01), Sneh
patent: 6468924 (2002-10-01), Lee et al.
patent: 6475276 (2002-11-01), Elers et al.
patent: 6475286 (2002-11-01), Frijlink
patent: 6475910 (2002-11-01), Sneh
patent: 6482262 (2002-11-01), Elers
patent: 6482476 (2002-11-01), Liu
patent: 6534395 (2003-03-01), Werkhoven et al.
patent: 6585823 (2003-07-01), Van Wijck
patent: 6586343 (2003-07-01), Ho et al.
patent: 6589886 (2003-07-01), Kim et al.
patent: 6590251 (2003-07-01), Kang et al.
patent: 6602784 (2003-08-01), Sneh
patent: 6613587 (2003-09-01), Carpenter et al.
patent: 6613695 (2003-09-01), Pomarede et al.
patent: 6620253 (2003-09-01), Dando et al.
patent: 6620723 (2003-09-01), Byun
patent: 6630401 (2003-10-01), Sneh
patent: 6638862 (2003-10-01), Sneh
patent: 6664192 (2003-12-01), Satta et al.
patent: 6673701 (2004-01-01), Marsh et al.
patent: 6696157 (2004-02-01), David
patent: 6696368 (2004-02-01), Derraa et al.
patent: 6720027 (2004-04-01), Yang et al.
patent: 6727169 (2004-04-01), Raaijmakers et al.
patent: 6730367 (2004-05-01), Sandhu
patent: 6746952 (2004-06-01), Derraa et al.
patent: 6753271 (2004-06-01), Sarigiannis et al.
patent: 6821347 (2004-11-01), Carpenter et al.
patent: 2001/0024387 (2001-09-01), Raaijmakers et al.
patent: 2001/0041250 (2001-11-01), Werkhoven et al.
patent: 2001/0050039 (2001-12-01), Park
patent: 2001/0054381 (2001-12-01), Umotoy et al.
patent: 2002/0086111 (2002-07-01), Byun et al.
patent: 2002/0108570 (2002-08-01), Lindfors
patent: 2002/0108714 (2002-08-01), Doering et al.
patent: 2002/0173054 (2002-11-01), Kim
patent: 2002/0173130 (2002-11-01), Pomerede et al.
patent: 2002/0187256 (2002-12-01), Elers
patent: 2003/0031807 (2003-02-01), Elers et al.
patent: 2003/0032281 (2003-02-01), Werkhoven et al.
patent: 2003/0082307 (2003-05-01), Chung et al.
patent: 2003/0085424 (2003-05-01), Bryant et al.
patent: 2003/0108674 (2003-06-01), Chung et al.
patent: 2003/0129826 (2003-07-01), Werkhoven et al.
patent: 2003/0143328 (2003-07-01), Chen et al.
patent: 2003/0183171 (2003-10-01), Sneh et al.
patent: 2004/0033688 (2004-02-01), Sarigiannis et al.
patent: 2004/0083959 (2004-05-01), Carpenter et al.
patent: 2004/0137728 (2004-07-01), Gallagher et al.
patent: 2005/0037597 (2005-02-01), Nguyen et al.
patent: 2006/0265100 (2006-11-01), Li
patent: WO 01/27347 (2001-04-01), None
patent: WO 01/29280 (2001-04-01), None
patent: WO 01/29893 (2001-04-01), None
patent: WO 01/66832 (2001-09-01), None
patent: PCT/US03/22804 (2003-07-01), None
patent: WO 2004/011693 (2004-02-01), None
U.S. Appl. No. 10/132,003, Dando.
U.S. Appl. No. 10/132,767, Dando.
U.S. Appl. No. 10/150,388, Mardian et al.
U.S. Appl. No. 10/163,689, Derderian et al.
U.S. Appl. No. 10/208,314, Castrovillo et al.
U.S. Appl. No. 10/222,304, Sarigiannis et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Atomic layer deposition methods does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Atomic layer deposition methods, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Atomic layer deposition methods will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2765933

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.