ABSTRACT:
This invention includes atomic layer deposition methods of depositing oxide comprising layers on substrates. In one implementation, a substrate is positioned within a deposition chamber. A first species is chemisorbed to form a first species monolayer onto the substrate within the deposition chamber from a gaseous first precursor. The chemisorbed first species is contacted with a gaseous second precursor effective to react with the first species to form an oxide of a component of the first species monolayer. The contacting at least in part results from flowing O3to the deposition chamber, with the O3being at a temperature of at least 170° C. at a location where it is emitted into the deposition chamber. The chemisorbing and the contacting are successively repeated to form an oxide comprising layer on the substrate. Additional aspects and implementations are contemplated.
REFERENCES:
patent: 4949671 (1990-08-01), Davis et al.
patent: 6403414 (2002-06-01), Marsh
patent: 6451692 (2002-09-01), Derderian et al.
patent: 6454912 (2002-09-01), Ahn et al.
patent: 6495458 (2002-12-01), Marsh
patent: 6534357 (2003-03-01), Basceri et al.
patent: 6596583 (2003-07-01), Agarwal et al.
patent: 6613656 (2003-09-01), Li
patent: 2003/0207540 (2003-11-01), Ahn et al.
patent: 2003/0207593 (2003-11-01), Derderian et al.
patent: 2003/0227033 (2003-12-01), Ahn et al.
patent: 2003/0232511 (2003-12-01), Metzner et al.
Derderian Garo J.
Meng Shuang
Sarigiannis Demetrius
Ghyka Alexander
Wells St. John P.S.
LandOfFree
Atomic layer deposition method of forming an oxide... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Atomic layer deposition method of forming an oxide..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Atomic layer deposition method of forming an oxide... will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-3699283