Atomic layer deposition apparatus

Data processing: generic control systems or specific application – Specific application – apparatus or process – Product assembly or manufacturing

Reexamination Certificate

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C438S478000, C118S719000, C118S729000

Reexamination Certificate

active

07085616

ABSTRACT:
A method and apparatus for atomic layer deposition (ALD) is described. The apparatus comprises a deposition chamber and a wafer support. The deposition chamber is divided into two or more deposition regions that are integrally connected one to another. The wafer support is movable between the two or more interconnected deposition regions within the deposition chamber.

REFERENCES:
patent: 4058430 (1977-11-01), Suntola et al.
patent: 4389973 (1983-06-01), Suntola et al.
patent: 4413022 (1983-11-01), Suntola et al.
patent: 4415275 (1983-11-01), Dietrich
patent: 4423701 (1984-01-01), Nath et al.
patent: 4486487 (1984-12-01), Skarp
patent: 4664939 (1987-05-01), Ovshinsky
patent: 4761269 (1988-08-01), Conger et al.
patent: 4767494 (1988-08-01), Kobayashi et al.
patent: 4806321 (1989-02-01), Nishizawa et al.
patent: 4813846 (1989-03-01), Helms
patent: 4829022 (1989-05-01), Kobayashi et al.
patent: 4834831 (1989-05-01), Nishizawa et al.
patent: 4838983 (1989-06-01), Schumaker et al.
patent: 4838993 (1989-06-01), Aoki et al.
patent: 4840921 (1989-06-01), Matsumoto
patent: 4845049 (1989-07-01), Sunakawa
patent: 4859307 (1989-08-01), Nishizawa et al.
patent: 4859627 (1989-08-01), Sunakawa
patent: 4861417 (1989-08-01), Mochizuki et al.
patent: 4876218 (1989-10-01), Pessa et al.
patent: 4917556 (1990-04-01), Stark et al.
patent: 4927670 (1990-05-01), Erbil
patent: 4931132 (1990-06-01), Aspnes et al.
patent: 4951601 (1990-08-01), Maydan et al.
patent: 4960720 (1990-10-01), Shimbo
patent: 4975252 (1990-12-01), Nishizawa et al.
patent: 4993357 (1991-02-01), Scholz
patent: 5000113 (1991-03-01), Wang et al.
patent: 5013683 (1991-05-01), Petroff et al.
patent: 5027746 (1991-07-01), Frijlink et al.
patent: 5028565 (1991-07-01), Chang et al.
patent: 5082798 (1992-01-01), Arimoto
patent: 5085885 (1992-02-01), Foley et al.
patent: 5091320 (1992-02-01), Aspnes et al.
patent: 5130269 (1992-07-01), Kitahara et al.
patent: 5166092 (1992-11-01), Mochizuki et al.
patent: 5173327 (1992-12-01), Sandhu et al.
patent: 5173474 (1992-12-01), Connell et al.
patent: 5186718 (1993-02-01), Tepman et al.
patent: 5205077 (1993-04-01), Wittstock
patent: 5225366 (1993-07-01), Yoder
patent: 5234561 (1993-08-01), Randhawa et al.
patent: 5246536 (1993-09-01), Nishizawa et al.
patent: 5250148 (1993-10-01), Nishizawa et al.
patent: 5254207 (1993-10-01), Nishizawa et al.
patent: 5256244 (1993-10-01), Ackerman
patent: 5259881 (1993-11-01), Edwards et al.
patent: 5261959 (1993-11-01), Gasworth
patent: 5270247 (1993-12-01), Sakuma et al.
patent: 5278435 (1994-01-01), Van Hove et al.
patent: 5281274 (1994-01-01), Yoder
patent: 5286296 (1994-02-01), Sato et al.
patent: 5290748 (1994-03-01), Knuuttila et al.
patent: 5294286 (1994-03-01), Nishizawa et al.
patent: 5296403 (1994-03-01), Nishizawa et al.
patent: 5300186 (1994-04-01), Kitahara et al.
patent: 5311055 (1994-05-01), Goodman et al.
patent: 5316615 (1994-05-01), Copel
patent: 5316793 (1994-05-01), Wallace et al.
patent: 5330610 (1994-07-01), Eres et al.
patent: 5336324 (1994-08-01), Stall et al.
patent: 5338362 (1994-08-01), Imahashi
patent: 5338389 (1994-08-01), Nishizawa et al.
patent: 5348911 (1994-09-01), Jurgensen et al.
patent: 5374570 (1994-12-01), Nasu et al.
patent: 5384008 (1995-01-01), Sinha et al.
patent: 5395791 (1995-03-01), Cheng et al.
patent: 5438952 (1995-08-01), Otsuka
patent: 5439876 (1995-08-01), Graf et al.
patent: 5441703 (1995-08-01), Jurgensen
patent: 5443033 (1995-08-01), Nishizawa et al.
patent: 5443647 (1995-08-01), Aucoin et al.
patent: 5455072 (1995-10-01), Bension et al.
patent: 5458084 (1995-10-01), Thorne et al.
patent: 5469806 (1995-11-01), Mochizuki et al.
patent: 5480818 (1996-01-01), Matsumoto et al.
patent: 5483919 (1996-01-01), Yokoyama et al.
patent: 5484664 (1996-01-01), Kitahara et al.
patent: 5503875 (1996-04-01), Imai et al.
patent: 5518542 (1996-05-01), Matsukawa et al.
patent: 5521126 (1996-05-01), Okamura et al.
patent: 5527733 (1996-06-01), Nishizawa et al.
patent: 5532511 (1996-07-01), Nishizawa et al.
patent: 5540783 (1996-07-01), Eres et al.
patent: 5580380 (1996-12-01), Liu et al.
patent: 5601651 (1997-02-01), Watabe
patent: 5609689 (1997-03-01), Kato et al.
patent: 5616181 (1997-04-01), Yamamoto et al.
patent: 5637530 (1997-06-01), Gaines et al.
patent: 5641984 (1997-06-01), Aftergut et al.
patent: 5644128 (1997-07-01), Wollnik et al.
patent: 5667592 (1997-09-01), Boitnott et al.
patent: 5674786 (1997-10-01), Turner et al.
patent: 5693139 (1997-12-01), Nishizawa et al.
patent: 5695564 (1997-12-01), Imahashi
patent: 5705224 (1998-01-01), Murota et al.
patent: 5707880 (1998-01-01), Aftergut et al.
patent: 5711811 (1998-01-01), Suntola et al.
patent: 5730801 (1998-03-01), Tepman et al.
patent: 5730802 (1998-03-01), Ishizumi et al.
patent: 5747113 (1998-05-01), Tsai
patent: 5749974 (1998-05-01), Habuka et al.
patent: 5788447 (1998-08-01), Yonemitsu et al.
patent: 5788799 (1998-08-01), Steger et al.
patent: 5796116 (1998-08-01), Nakata et al.
patent: 5801634 (1998-09-01), Young et al.
patent: 5807792 (1998-09-01), Ilg et al.
patent: 5830270 (1998-11-01), McKee et al.
patent: 5835677 (1998-11-01), Li et al.
patent: 5851849 (1998-12-01), Comizzoli et al.
patent: 5855675 (1999-01-01), Doering et al.
patent: 5855680 (1999-01-01), Soininen et al.
patent: 5856219 (1999-01-01), Naito et al.
patent: 5858102 (1999-01-01), Tsai
patent: 5866213 (1999-02-01), Foster et al.
patent: 5866795 (1999-02-01), Wang et al.
patent: 5879459 (1999-03-01), Gadgil et al.
patent: 5882165 (1999-03-01), Maydan et al.
patent: 5882413 (1999-03-01), Beaulieu et al.
patent: 5904565 (1999-05-01), Nguyen et al.
patent: 5916365 (1999-06-01), Sherman
patent: 5923056 (1999-07-01), Lee et al.
patent: 5923985 (1999-07-01), Aoki et al.
patent: 5925574 (1999-07-01), Aoki et al.
patent: 5928389 (1999-07-01), Jevtic
patent: 5942040 (1999-08-01), Kim et al.
patent: 5947710 (1999-09-01), Cooper et al.
patent: 5972430 (1999-10-01), DiMeo, Jr. et al.
patent: 6001669 (1999-12-01), Gaines et al.
patent: 6015590 (2000-01-01), Suntola et al.
patent: 6025627 (2000-02-01), Forbes et al.
patent: 6026589 (2000-02-01), Yao et al.
patent: 6036773 (2000-03-01), Wang et al.
patent: 6042652 (2000-03-01), Hyun et al.
patent: 6043177 (2000-03-01), Falconer et al.
patent: 6051286 (2000-04-01), Zhao et al.
patent: 6062798 (2000-05-01), Muka
patent: 6071572 (2000-06-01), Mosely et al.
patent: 6071808 (2000-06-01), Merchant et al.
patent: 6084302 (2000-07-01), Sandhu
patent: 6086677 (2000-07-01), Umotoy et al.
patent: 6110556 (2000-08-01), Bang et al.
patent: 6113977 (2000-09-01), Soininen et al.
patent: 6117244 (2000-09-01), Bang et al.
patent: 6124158 (2000-09-01), Dautartas et al.
patent: 6130147 (2000-10-01), Major et al.
patent: 6139695 (2000-10-01), Washburn et al.
patent: 6139700 (2000-10-01), Kang et al.
patent: 6140237 (2000-10-01), Chan et al.
patent: 6140238 (2000-10-01), Kitch
patent: 6143082 (2000-11-01), McInerney et al.
patent: 6143659 (2000-11-01), Leem
patent: 6144060 (2000-11-01), Park et al.
patent: 6158446 (2000-12-01), Mohindra et al.
patent: 6174377 (2001-01-01), Doering et al.
patent: 6174809 (2001-01-01), Kang et al.
patent: 6178660 (2001-01-01), Emmi et al.
patent: 6183563 (2001-02-01), Choi et al.
patent: 6197683 (2001-03-01), Kang et al.
patent: 6200441 (2001-03-01), Gornicki et al.
patent: 6200893 (2001-03-01), Sneh
patent: 6203613 (2001-03-01), Gates et al.
patent: 6206967 (2001-03-01), Mak et al.
patent: 6207302 (2001-03-01), Sugiura et al.
patent: 6231672 (2001-05-01), Choi et al.
patent: 6248605 (2001-06-01), Harkonen et al.
patent: 6270572 (2001-08-01), Kim et al.
patent: 6271148 (2001-08-01), Kao et al.
patent: 6281098 (2001-08-01), Wang et al.
patent: 6287965 (2001-09-01), Kang et al.
patent: 6291876 (2001-09-01), Stumborg et al.
patent: 6302965 (2001-10-01), Umotoy et al.
patent: 6305314 (2001-10-01), Sneh et al.
patent: 6306216 (2001-10-01), Kim et al.
patent: 6316098 (2001-11-01), Yitzchaik et al.
patent: 6319553 (2001-11-01), McInerney et al.
patent: 6342277 (2002-01-01), Sherman
patent: 6365025 (2002-04-01), Ting et al.
patent: 6387185 (2002-05-01), Do

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Atomic layer deposition apparatus does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Atomic layer deposition apparatus, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Atomic layer deposition apparatus will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3628893

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.