ABSTRACT:
A method for making large scale integrated circuits on a disklike semiconductor substrate includes grinding a disk thin enough to be able to be sawn apart into individual chips. A damage zone caused by the grinding on a back side of the wafer is removed by etching while protecting a front side of the wafer, prior to sawing. The etching is carried out in the form of a microwave or high-frequency-excited downstream plasma etching process using fluorine compounds in an etching gas.

REFERENCES:
patent: 4946547 (1990-08-01), Palmour et al.
patent: 5075256 (1991-12-01), Wang et al.
Patent Abstract of Japan No. JP 3-272140 (Otake), Dec. 3, 1991.
IEEE Publ., vol. 13, No.3, Sep. 1990, Nishiguchi et al., pp.528-533, "Mass Production Back-Grinding/Wafer-Thinning Technology for GaAs Dev."
American Institute of Physics Publ. 54 (25), 9 Jun. 1989, pp. 2553-2555, (Ohkawa et al.) "Homoepitaxial growth of ZnSe on dry-etched substrates".
Solid State Technology Publ. Oct. 1994, (Boitnott), pp. 51,52,56,58, "Downstream Plasma Processing: Consideration for selective etch and other process".
Motorla, Inc. Publ. vol. 23, Oct. 1994, (Shumate et al.), p. 8, "Silicon Wafer Thinning and Dicing Round or Non Orthogonal Die Using Dry Etching".

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for damage etching the back side of a semiconductor disk does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for damage etching the back side of a semiconductor disk , we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for damage etching the back side of a semiconductor disk will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-798175

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.