Method of making a smooth, dimensionally stable, mica-filled, gl

Paper making and fiber liberation – Processes and products – With coating after drying

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

162145, 162146, 162168R, 162169, 162181C, 428283, 428324, 428363, 428454, B32B 516, D21F 1100

Patent

active

042473640

ABSTRACT:
A mica-filled glass fiber sheet which is smooth, of relatively low porosity, and dimensionally stable is described as is its method of manufacture. The sheet is prepared from a low-consistency aqueous slurry wherein the solids consist essentially of glass fibers, organic fibers, mica, and binder. Based on 100 parts by weight glass fibers, 3 to 15 parts by weight organic fibers, 30 to 100 parts by weight mica flakes, and 5 to 20 parts by weight organic binder are added to the water in preparing the furnish. In forming the sheet, this slurry or furnish is deposited onto a moving screen, the excess water is removed, and the wet laid sheet is dried and the binder set. In a subsequent operation, the sheet is saturated with a resin solution or latex.

REFERENCES:
patent: 2917426 (1959-12-01), Bugosh
patent: 3017318 (1962-01-01), Labino et al.
patent: 3039914 (1962-06-01), Reiman
patent: 3080272 (1963-03-01), Jackson
patent: 3108926 (1963-10-01), Brown
patent: 3344016 (1967-09-01), Moggio et al.
patent: 3622445 (1971-11-01), Heidweiller
patent: 3679544 (1972-07-01), Ashikaga et al.
patent: 3749638 (1973-07-01), Renaud et al.
patent: 3773513 (1973-11-01), MacClaren
patent: 4060451 (1977-11-01), Uchiyama et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of making a smooth, dimensionally stable, mica-filled, gl does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of making a smooth, dimensionally stable, mica-filled, gl, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of making a smooth, dimensionally stable, mica-filled, gl will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1180275

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.