Semiconductor device manufacturing: process – Packaging or treatment of packaged semiconductor
Reexamination Certificate
2002-03-20
2003-07-01
Talbott, David L. (Department: 2827)
Semiconductor device manufacturing: process
Packaging or treatment of packaged semiconductor
C438S108000, C438S612000, C257S780000, C257S779000, C257S778000, C257S620000
Reexamination Certificate
active
06586275
ABSTRACT:
BACKGROUND OF THE INVENTION
1. Field of the Invention
The present invention generally relates to the field of semiconductor manufacturing and, more particularly, to a wafer level package (WLP) with improved interconnection reliability and a method for manufacturing the same.
2. Description of the Related Art
In order to meet ever-demanding packaging requirements for newer generations of electronic products, countless efforts have been expended to create the most reliable, cost-effective, small, and high-performance packages. Such requirements are, for example, reductions in propagation delay and in overall component area as well as broader latitude in input/output (I/O).
To meet those requirements, a wafer level package (WLP) has been recently developed. In the WLP, unlike the periphery leaded packages, an array of external terminals is distributed over the semiconductor surface in place of outer leads of leaded packages. This reduces the signal path from a semiconductor chip to package I/O location, thereby improving the electrical performance of the device. Further, the area it occupies when mounted onto a printed circuit board or other substrate is the size of the chip. Thus, the size of the WLP is very small.
For these reasons, almost all WLPs use metallic solder balls disposed in an area array fashion to interconnect the package to the printed circuit board.
However, due to grossly mismatched coefficient of thermal expansions (CTE) between the chip and the printed circuit board, if the metallic solder balls, which are minimally elastic, alone were used to interconnect the chip contacts to the substrate, the strain would be absorbed by the solder balls, causing them to crack and fail due to the mechanical stress of the differential CTE of the chip relative to the printed circuit board, thereby damaging the reliability of the solder connection.
In other words, when the chip heats up during use, both the chip and the board expand, and when the heat is removed, both the chip and the substrate shrink. The problem that arises is that the chip and the substrate expand and contract at different rates and at different times, thereby stressing the interconnections or solder balls between them.
Some attempts have been made to solve these problems, but they turned out to be unsuccessful. Moreover, if the chip size becomes large, it has been discovered that the residual stress or displacement at the periphery of the chip also significantly increases compared to that of the center portion of the chip.
As a result, with conventional structures, experience says that it is not sufficient to prevent the solder cracking or the breakage of metal interconnection at the side of the solder ball pad, especially near the edge of the chip.
Therefore, what is needed is a newly designed WLP with improved interconnection reliability, especially between the chip and the board, and a method of manufacturing the same.
SUMMARY OF THE INVENTION
The present invention provides a thermal-stress-absorbing interface structure for a WLP and the method of manufacturing the same to improve interconnection reliability of the WLP such as solder joint reliability.
According to preferred embodiments of the present invention, a thermal-stress-absorbing interface structure between a semiconductor integrated circuit chip and a surface-mount structure comprises an elongated conductive-bump pad having a first length-wise end and a second length-wise end, and a side. The thermal-stress-absorbing interface structure further includes means for allowing the first end of the pad to move up when the second end of the pad moves down and alternately allowing the first end to move down when the second end moves up, upon thermal cycling. The means has a center axis. The up-and-down movements of the pad are balanced on the center axis. The interface structure can include a conductive bump formed on the pad.
According one aspect of the present invention, a method of forming a WLP is disclosed. The method comprises providing a semiconductor wafer having a plurality of semiconductor chips and a plurality of scribe lines. Each of the semiconductor chips includes a plurality chip pads and a passivation layer thereon. Then, a multi-layer thermal-stress-absorbing support structure is formed over the resulting structure. Next, a first patterned conductor layer is formed over the multi-layer structure. A first patterned insulation layer is formed over the first patterned conductor layer. Here, the first patterned insulation layer includes an opening therein. The opening exposes a portion of the first patterned conductor layer. Then, a conductive bump is placed over the exposed portion of first patterned conductor layer. Lastly, the wafer is singulated to separate the semiconductor chips to complete the WLP.
Preferably, the multi-layer structure comprises a first polymer layer and a second polymer layer covering the first polymer layer. The first and second polymer layers and the pad including the interconnection line, which extends from the side thereof intermediate the first and the second ends, cooperatively allows the elongated conductive bump pad to make the up-and-down movements pivoted on the center axis and allows the first and second polymers to resiliently deform corresponding to the up-and-down movements of the pad balanced on the center axis, upon thermal cycling. This absorbs or dissipates thermal stresses generated during thermal cycling.
With these features of the present invention, interconnection reliability of the WLP can be significantly improved. For example, the thermal stresses generated during the thermal cycling are absorbed or dissipated efficiently without breakage of the joints (physical connection) between the conductive bump and the underlying structure.
The foregoing and other objects, features and advantages of the invention will become more readily apparent from the following detailed description of a preferred embodiment of the invention that proceeds with reference to the accompanying drawings.
REFERENCES:
patent: 5679977 (1997-10-01), Khandros et al.
patent: 5780933 (1998-07-01), Ohmori et al.
patent: 5852326 (1998-12-01), Khandros et al.
patent: 6022763 (2000-02-01), Ohmori et al.
patent: 6277669 (2001-08-01), Kung et al.
Semyon Vaynman, et al. “Energy-Based Methodology for the Fatigue Life Prediction of Solder Materials”IEEE Transactions On Components, Hybrids, and Manufacturing Technology, vol. 16, No. 3, pp. 317-322, May 1993.
Jang Dong-Hyeon
Kang Sa-Yoon
Kim Gu-Sung
Son Min-Young
Marger & Johnson & McCollom, P.C.
Samsung Electronics Co,. Ltd.
Talbott David L.
Thai Luan
LandOfFree
Wafer level package and method for manufacturing the same does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Wafer level package and method for manufacturing the same, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Wafer level package and method for manufacturing the same will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-3037782