Thin cast steel strip with reduced microcracking

Metal founding – Process – Shaping liquid metal against a forming surface

Reexamination Certificate

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C164S428000

Reexamination Certificate

active

07975754

ABSTRACT:
A thin cast steel strip and method of making thereof with improved resistance to microcracking, where the steel strip is produced by continuous casting and contains a carbon content between about 0.010% and about 0.065% by weight, less than 5.0% by weight chromium, at least 70 ppm of total oxygen and between 20 and 70 ppm of free oxygen, and manganese to sulfur ratio greater than about 250. The carbon content in the cast strip may be below about 0.035%, less than 0.005% by weight titanium, and the average manganese to silicon ratio in the strip produced may be greater than 3.5. The carbon content may be less than 0.035%, the casting speed less than 76.68 meters per minute, and the tundish temperature of the molten metal is maintained below 1612° C. (2933.7° F.).

REFERENCES:
patent: 5063990 (1991-11-01), Follstaedt et al.
patent: 5297614 (1994-03-01), Bessho et al.
patent: 5390726 (1995-02-01), Fukuda et al.
patent: 5807444 (1998-09-01), Paradis et al.
patent: 5901777 (1999-05-01), Matsumura et al.
patent: 5934359 (1999-08-01), Strezov
patent: 6059014 (2000-05-01), Strezov
patent: 6386271 (2002-05-01), Kawamoto et al.
patent: 6491089 (2002-12-01), Poirier et al.
patent: 6588494 (2003-07-01), Mazurier et al.
patent: 6622779 (2003-09-01), Mazurier
patent: 6679313 (2004-01-01), Poirier et al.
patent: 6739383 (2004-05-01), Marchionni et al.
patent: 7117925 (2006-10-01), Strezov et al.
patent: 7156151 (2007-01-01), Mahapatra et al.
patent: 7296614 (2007-11-01), Schlichting et al.
patent: 2005/0082031 (2005-04-01), Mahapatra et al.
patent: 2006/0191612 (2006-08-01), Yoshida et al.
patent: 2007/0144632 (2007-06-01), Toyoda et al.
patent: 2007/0175608 (2007-08-01), Mahapatra et al.
patent: 03-248750 (1991-11-01), None
patent: 03-294419 (1991-12-01), None
patent: 04-045223 (1992-02-01), None
patent: 07-314097 (1995-12-01), None
patent: 08-192250 (1996-07-01), None
patent: 270147 (1994-12-01), None
patent: 02/028569 (2002-04-01), None
patent: 03/024644 (2003-03-01), None
PCT/AU2008/001164 Further Written Opinion.
PCT/AU2008/001164 International Search Report.
PCT/AU2008/001164 Written Opinion.
AU2008900484 Search Report.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Thin cast steel strip with reduced microcracking does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Thin cast steel strip with reduced microcracking, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Thin cast steel strip with reduced microcracking will most certainly appreciate the feedback.