ABSTRACT:
A finless mortar tube made of a superalloy includes, seriatim, a breech end, a beginning taper point, an ending taper point, a lower clamp region, an upper clamp region, and a muzzle end. The nominal wall thickness of the tube is constant from forward of the breech end to the beginning taper point and the nominal wall thickness of the tube decreases from the beginning taper point to the ending taper point. The mortar tube is capable of a substantial increase in the rate of fire compared to conventional mortar tubes.
REFERENCES:
patent: 1346188 (1920-07-01), Fahrenwald
patent: 1365987 (1921-01-01), Hadfield et al.
patent: 1384718 (1921-07-01), Guy
patent: 1553825 (1925-09-01), Langenberg
patent: 2541114 (1951-02-01), Somes
patent: 2541116 (1951-02-01), Somes
patent: 2876095 (1959-03-01), Dickerson
patent: 2990342 (1961-06-01), Sullivan
patent: 3516326 (1970-06-01), Donner
patent: 3892163 (1975-07-01), Asikainen
patent: 4146077 (1979-03-01), Klein et al.
patent: 4198897 (1980-04-01), Lipp et al.
patent: 4417459 (1983-11-01), Tomita
patent: 4571969 (1986-02-01), Tomita
patent: 4646615 (1987-03-01), Gladstone et al.
patent: 4669212 (1987-06-01), Jackson et al.
patent: 4747225 (1988-05-01), Gstettner et al.
patent: 4756677 (1988-07-01), Hribernik et al.
patent: 5160802 (1992-11-01), Moscrip
patent: 5305679 (1994-04-01), Begneu
patent: 5341719 (1994-08-01), Bullis et al.
patent: 5429032 (1995-07-01), Cytron
patent: 5531150 (1996-07-01), Gegaregian et al.
patent: 5677507 (1997-10-01), Becker et al.
patent: 5856631 (1999-01-01), Julien
patent: 5928799 (1999-07-01), Sherman et al.
patent: 5935351 (1999-08-01), Sherman et al.
patent: 6059573 (2000-05-01), Patel
patent: 6298764 (2001-10-01), Sherman et al.
patent: 6615702 (2003-09-01), Julien
patent: 6851348 (2005-02-01), Ang
patent: 6912945 (2005-07-01), Ang
patent: 7182014 (2007-02-01), Smith
patent: 7421934 (2008-09-01), Madulka et al.
patent: 7601232 (2009-10-01), Fonte et al.
patent: 7735408 (2010-06-01), Becker et al.
patent: 2001/0006018 (2001-07-01), Ang
patent: 2005/0034346 (2005-02-01), Smith
patent: 2006/0288854 (2006-12-01), Witherell et al.
patent: 2007/0221051 (2007-09-01), Burkholder et al.
patent: 2010/0236122 (2010-09-01), Fonte
Gourley, Scott, Mortar Technology, Special Operations Technology, 2008. http://www.special-operations-technology.com/sotech-home/176-sotech-2008-volume-5-issue-4/1640-mortar-technology.html.
Douglas, Richard, et al. Production of Inconel 718 Mortar Tubes By Hydrostatic Extrusion, Watervliet Arsenal, Watervliet, Niew York, Jul. 1974.
M224 60mm Lightweight Mortar, 1999. http—web.archive.org—web—19991221083851—http—www.biggerhammer.net—factfile.nsf—ffiles—a072707cfe330d3b8525627b006b6e36.pdf.
M224 60-MM Mortar Basis of Issue Plan, 2000. http—web.archive.org—web—20000530071510—http—www.fas.org—man—dod-101—sys—land—docs—bnl005AA.pdf.
M224 60mm Lightweight Company Mortar System, 2003. http—web.archive.org—web—20030219151349—http—www.fas.org—man—dod-101—sys—land—m224.pdf.
National Defense Industrial Association, Picatinny Chapter, vol. 1, Issue V. Nov. 2005. http—www.ndiapicatinny.com—downloads—2005—Nov%2005%20Newsletter.pdf.
The Voice, 2005. http—www.pica.army.mil—voice—voice2005—051202—051202%20Mortar%20conf.pdf.
KMI Media Group, 2011.http—www.special-operations-technology.com—component—search—searchword=superalloy&ordering=&searchphrase=all.pdf.
Kemp, Ian, Infantry: Mortars, Armada International (Accessed at The Free Library.com) Apr. 1, 2006. http—www.thefreelibrary.com—Pocket+artillery.-a0146354592.pdf.
Patriarca, Michael, Innovation Drives Lightweight Mortar Weapon System Development, USAASC, Jan. 2008. http—www.usaasc.info—alt—online—article.cfm—ilD=0801&aid=10.pdf.
Becker Richard F.
Espinosa Ramon
Hathaway, IV George E.
Santiago Jose
Tauscher Steve
Clement Michelle
Moran John F
The United States of America as represented by the Secretary of
LandOfFree
Superalloy mortar tube does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Superalloy mortar tube, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Superalloy mortar tube will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2626636