Semi-hard magnetic elements formed by annealing and controlled o

Communications: electrical – Condition responsive indicating system – Specific condition

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

148561, 420125, 420590, 340572, G08B 13187, H01F 1153

Patent

active

057677700

ABSTRACT:
A semi-hard magnetic element is formed by at least partially crystallizing an amorphous soft iron-metalloid material. The heating process used to achieve crystallization includes a controlled oxidation stage to increase the level of remanent flux that is provided when the processed magnetic element is placed in a fully magnetized state.

REFERENCES:
patent: 4510489 (1985-04-01), Anderson, III et al.
patent: 4510490 (1985-04-01), Anderson, III et al.
patent: 5252144 (1993-10-01), Martis
patent: 5351033 (1994-09-01), Liu et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Semi-hard magnetic elements formed by annealing and controlled o does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Semi-hard magnetic elements formed by annealing and controlled o, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Semi-hard magnetic elements formed by annealing and controlled o will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1730657

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.