Roughening surface of a substrate

Adhesive bonding and miscellaneous chemical manufacture – Delaminating processes adapted for specified product – Delaminating in preparation for post processing recycling step

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

156646, 156655, 156668, 156902, 252 791, 427 96, 427 98, 427307, B44C 122, C03C 1500, C03C 2506, B29C 1708

Patent

active

046157638

ABSTRACT:
The surface of a substrate is roughened by providing a substrate which comprises a resinous material and an inorganic particulate material; and etching a surface of the substrate to selectively etch the resinous material and thereby produce the roughened surface.

REFERENCES:
patent: 2663663 (1953-12-01), Weltman et al.
patent: 3625758 (1971-12-01), Stahl et al.
patent: 3795557 (1974-03-01), Jacob
patent: 3801427 (1974-04-01), Morishita et al.
patent: 3884771 (1975-05-01), Hanabusa et al.
patent: 3978252 (1976-08-01), Lombardo et al.
patent: 4113899 (1978-09-01), Henry et al.
patent: 4147564 (1979-04-01), Magee et al.
patent: 4152477 (1979-05-01), Haruta et al.
patent: 4180432 (1979-12-01), Clark
patent: 4216246 (1980-08-01), Iwasaki et al.
patent: 4281038 (1981-07-01), Ambros et al.
patent: 4283249 (1981-08-01), Ephrath
patent: 4325991 (1982-04-01), Donovan
patent: 4469777 (1984-09-01), O'Neil
IBM Technical Disclosure Bulletin, vol. 26, No. 2, Jul. 1983, Method of Improving the Adhesive of Copper on a Plastic Laminate, H. Bohlen, pp. 673-674.
Robin H. Wheater et al., "Polymer Interlayer Adhesion Enhancements Through Plasma Surface Modification".

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Roughening surface of a substrate does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Roughening surface of a substrate, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Roughening surface of a substrate will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-641629

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.