ABSTRACT:
A method of recovering rhenium from rhenium-containing superalloy scrap is provided. The superalloy is usually a nickel-based superalloy. The method includes the steps of forming an oxidation feedstock of flaky morphology of the superalloy scrap, and oxidizing the oxidation feedstock to convert rhenium into a volatile rhenium oxide. The flaky morphology of the oxidation feedstock is achieved by increasing the surface area of the superalloy scrap.
REFERENCES:
patent: 2848313 (1958-08-01), Takahashi et al.
patent: 4604265 (1986-08-01), Douglas et al.
patent: 4787561 (1988-11-01), Kemp et al.
patent: 4880170 (1989-11-01), Kemp et al.
patent: 5482789 (1996-01-01), O'Hara et al.
patent: 5776329 (1998-07-01), Krynitz et al.
patent: 6131835 (2000-10-01), Johnson
patent: 6835365 (2004-12-01), Davies et al.
patent: 2003/0119658 (2003-06-01), Allison et al.
patent: 2003/0136685 (2003-07-01), Stoller et al.
patent: 2008/0216606 (2008-09-01), Marsden et al.
patent: 2009/0317288 (2009-12-01), Yokokawa et al.
patent: 2010/0180514 (2010-07-01), Liu
Nadler et al. “Rhenium and Rhenium Compounds”. Wiley-VCH Verlag GmgH & Co. KGaA, Weinheim. 2005.
Ferrante, M.J. et al “Recovery of Rhenium from Tungsten-Rhenium Alloy.” United States Bureau of Mines Report of Investigation No. 7022. Apr. 1969.
Drobot et al. “Recycling of Rhenium.” Rhenium and Rhenium Alloys, Proceedings of the International Symposium. pp. 119-127. Feb. 9-13, 1997.
A.V. Tarasov, V.M. Paretsky, A.D. Besser and E.I Gedgagov; Processing of Grinding Waste of Rhenium-Containing Alloys to Manufacture Commercial-Grade Metals; TMS ( The Minerals, Metals & Materials Society) 2008; pp. 1051-1059.
B. Heshmatpour and R.E. McDonald; Recovery and Refining of Rhenium, Tungsten and Molybdenum from W-Re, Mo-Re and Other Alloy Scraps; Journal of the Less-Common Metals, 86 (1982); pp. 121-128.
Ajdelsztajn Leonardo
Dasan Biju
Lipkin Don Mark
Miller Joshua Leigh
Palanisamy Barath
Coppa Francis T.
General Electric Company
McGuthry Banks Tima M
Wyszomierski George
LandOfFree
Rhenium recovery from superalloys and associated methods does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Rhenium recovery from superalloys and associated methods, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Rhenium recovery from superalloys and associated methods will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-4287686