ABSTRACT:
A method of recovering rhenium from rhenium-containing superalloy scrap is provided. The superalloy is usually a nickel-based superalloy. The method includes the steps of forming an oxidation feedstock of flaky morphology of the superalloy scrap, and oxidizing the oxidation feedstock to convert rhenium into a volatile rhenium oxide. The flaky morphology of the oxidation feedstock is achieved by increasing the surface area of the superalloy scrap.

REFERENCES:
patent: 2848313 (1958-08-01), Takahashi et al.
patent: 4604265 (1986-08-01), Douglas et al.
patent: 4787561 (1988-11-01), Kemp et al.
patent: 4880170 (1989-11-01), Kemp et al.
patent: 5482789 (1996-01-01), O'Hara et al.
patent: 5776329 (1998-07-01), Krynitz et al.
patent: 6131835 (2000-10-01), Johnson
patent: 6835365 (2004-12-01), Davies et al.
patent: 2003/0119658 (2003-06-01), Allison et al.
patent: 2003/0136685 (2003-07-01), Stoller et al.
patent: 2008/0216606 (2008-09-01), Marsden et al.
patent: 2009/0317288 (2009-12-01), Yokokawa et al.
patent: 2010/0180514 (2010-07-01), Liu
Nadler et al. “Rhenium and Rhenium Compounds”. Wiley-VCH Verlag GmgH & Co. KGaA, Weinheim. 2005.
Ferrante, M.J. et al “Recovery of Rhenium from Tungsten-Rhenium Alloy.” United States Bureau of Mines Report of Investigation No. 7022. Apr. 1969.
Drobot et al. “Recycling of Rhenium.” Rhenium and Rhenium Alloys, Proceedings of the International Symposium. pp. 119-127. Feb. 9-13, 1997.
A.V. Tarasov, V.M. Paretsky, A.D. Besser and E.I Gedgagov; Processing of Grinding Waste of Rhenium-Containing Alloys to Manufacture Commercial-Grade Metals; TMS ( The Minerals, Metals & Materials Society) 2008; pp. 1051-1059.
B. Heshmatpour and R.E. McDonald; Recovery and Refining of Rhenium, Tungsten and Molybdenum from W-Re, Mo-Re and Other Alloy Scraps; Journal of the Less-Common Metals, 86 (1982); pp. 121-128.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Rhenium recovery from superalloys and associated methods does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Rhenium recovery from superalloys and associated methods, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Rhenium recovery from superalloys and associated methods will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-4287686

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.