Refractory superalloys consist essentially of a primary constituent selected from the group consisting of iridium, rhodium, and a mixture thereof, and one or more additive elements selected from the group consisting of niobium, tantalum, hafnium, zirconium, uranium, vanadium, titanium and aluminum, and the superalloys having a microstructure containing an FCC-type crystalline structure phase and an L1.sub.2 -type crystalline structure phase are precipitated. Preferably the amount of additive element(s) is 2 to 22 atom %.
REFERENCES:
patent: 3918965 (1975-11-01), Inouye et al.
patent: 5080862 (1992-01-01), Luthra
patent: 5234774 (1993-08-01), Hasegawa et al.
Binary Alloy Phase Diagrams V2 ed by Thaddeus Massalski; Jun. 1987; pp. 1423-1424, 1430-1441, 1689, 1691, 1975, 1977, 1979-1981; 85 1986.
Harada Hiroshi
Koizumi Yutaka
Maruko Tomohiro
Murakami Hideyuki
Nakazawa Shizuo
National Research Institute for Metals
Yee Deborah
LandOfFree
Refractory superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Refractory superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Refractory superalloys will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2211026