ABSTRACT:
The removal of silica from an iron-bearing source which is treated to produce an iron powder which may be used in powder metallurgical applications may be facilitated by subjecting the reduced iron-bearing source such as magnetite to a sparge with an oxygen-containing gas such as oxygen or air prior to a caustic leach step. The sparge of the caustic-magnetite slurry is effected at ambient temperatures and pressures which may range from about 10 to about 1000 psi for a period of time ranging from about 0.1 to about 1 hour. By utilizing this sparge, the leaching capacity of the caustic leach solution appreciably increased.
REFERENCES:
patent: 4136158 (1979-01-01), Okuda et al.
patent: 4154608 (1979-05-01), Carey et al.
Hearn Brian E.
Hoatson Jr. James R.
Nelson Raymond H.
Page II William H.
Stoll Robert L.
LandOfFree
Process for the production of high purity iron powder does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for the production of high purity iron powder, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for the production of high purity iron powder will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1200466