ABSTRACT:
To reduce fouling on reactor surfaces, the surfaces are coated with a protective film of polymeric material of surface energy of less than 15 dynes/cm. The preferred coating materials are polymers of one or more monomer chosen from the 2-(N-alkylperfluorosulphonamido)) alkyl (meth)acrylates or the fluorochemical polymer known as Fluorad (Registered Trade Mark of the 3M company) FC-721.
REFERENCES:
patent: 4344993 (1982-08-01), Schmidt et al.
patent: 4604411 (1986-08-01), Yada et al.
patent: 4696983 (1987-09-01), Cohen
Polymer Handbook (2nd ed.), Wiley-Interscience, N.Y., III-221-227, 1975.
Crown Decorative Products Limited
Hinds William R.
Schofer Joseph L.
Teskin F. M.
LandOfFree
Process for reducing reactor fouling during polymerization in an does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for reducing reactor fouling during polymerization in an, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for reducing reactor fouling during polymerization in an will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1573248