ABSTRACT:
High concentrated coal-water slurry is produced by coarsely crushing coal, thereafter pulverizing the coarsely crushed coal, together with water and a slurry dispersant, according to necessity, in a wet-type ball mill, and feeding back one portion of the finely pulverized coal slurry thus obtained into the inlet of the wet-type ball mill.
REFERENCES:
patent: 1547491 (1925-07-01), Barthelmess
patent: 3715083 (1973-02-01), Funk
patent: 4062497 (1977-12-01), Kemp, Jr. et al.
patent: 4162045 (1979-07-01), Katzer et al.
patent: 4282006 (1981-08-01), Funk
Itoh Hayami
Kamao Mitsugu
Nakaoji Kazuhiko
Takao Shoichi
Tatsumi Shuhei
Electric Power Development Company Limited
Kao Corporation
Kawasaki Jukogyo Kabushiki Kaisha
Lion Corporation
Mitsui Engineering and Shipbuilding Company Limited
LandOfFree
Process for producing high-concentration slurry of coal does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for producing high-concentration slurry of coal, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for producing high-concentration slurry of coal will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-608828