ABSTRACT:
A diamond-coated tool and a process for making them. The process includes a sintering step. In that step, a substrate is sintered in an atmosphere and for a time and at a temperature so that superficial, exaggerated grain growth is promoted that imparts a surface roughness which may serve as anchoring sites during a subsequent diamond coating step which is performed by a vapor deposition technique. The diamond-coated tool or wear part includes a large grain substrate surface, and a high bond strength between the diamond coating and the substrate surface.
REFERENCES:
patent: Re34180 (1993-02-01), Nemeth et al.
patent: 4282289 (1981-08-01), Kullander et al.
patent: 4374685 (1983-02-01), Suzuki et al.
patent: 4636252 (1987-01-01), Yoshimura et al.
patent: 4643620 (1987-02-01), Fujii et al.
patent: 4690691 (1987-09-01), Komanduri
patent: 4731296 (1988-03-01), Kikuchi et al.
patent: 4755399 (1988-07-01), Fujii et al.
patent: 4843039 (1989-06-01), Akesson et al.
patent: 4985070 (1991-01-01), Kitamura et al.
patent: 4990403 (1991-02-01), Ito
patent: 5028451 (1991-07-01), Ito et al.
patent: 5066553 (1991-11-01), Yoshimura et al.
patent: 5068148 (1991-11-01), Nakahara et al.
patent: 5100703 (1992-03-01), Saijo et al.
patent: 5178645 (1993-01-01), Nakamura et al.
patent: 5204167 (1993-04-01), Saijo et al.
patent: 5370944 (1994-12-01), Omori et al.
patent: 5391422 (1995-02-01), Omori et al.
Yagi, M. et al., "Cutting Performance of Diamond Cutting Tool for A1-18 mass% Si Alloy," Journal of Japan, Institute of Light Metals, vol. 39, No. 6, pp. 417-422 (1989)(Trans. and Orig. Japanese).
Katsumura et al., "The Effects of Cobalt Content and Surface State of Substrate on Cutting Perfor-Performance of Diamond Deposited Cemented Carbide Tool for Al-18% Si Alloy," Journal of Japan, Institute of Light Metals, vol. 39, No. 9, pp. 634-638 (1989)(Trans. and Orig. Japanese).
ANSI B 46.1-1978, "Surface Texture" ASME (1978) pp. 1-37.
Saijo et al., "The Tool Life of Diamond Coatings in Milling an Al-Si Alloy," Applications of Diamond Films and Related Materials, ed. by Tzeng et al., Elsevier Sci. Pub. B.V. (1991), pp. 69-76.
Yagi, Masaru, "Cutting Performance of Diamond Deposited Tool on Al-18 mass% Si Alloy," Science and Technology of New Diamond, edited by S. Saito, O. Fukunaga and M. Yoshikawa, pp. 399-404, copyright by KTK Scientific Publishers, Terra Scientific Publishing Company, 1990.
Shibuki, Kunio; Yagi, Massaru; Saijo, Kosuke; & Takatsu, Sokichi, "Adhesion Strength of Diamond Films on Cemented Carbide Substrates," Surface & Coatings Technology, 36 (1988) pp. 295-302.
Craig, Phillip, Senior Editor, "Thin-Film-Diamond Derby," Cutting Tool Engineering, vol. 44, No. 1, Feb. 1992, Reprinted by Crystallume Engineered Diamond Products (6 pages).
Mason, Frederick, "Diamond: the Material of the Future," American Machinist, Feb. 1990, pp. 43-46.
Cyrstallume Engineered Diamond Products Brochure, "Engineering CVD Diamond for Extraordinary Performance in Demanding Applications," (1991) (7 pages).
Suzuki et al., "Diamond Deposition of WC-Co Cemented Carbide by Hot Filament Method," J. Jpn. Soc. Powder Metall., 33 (5) (1986) pp. 38-45) (English trans. and Japanese language copy).
Saito et al., "Adhesion of Diamond Film on Cemented Carbide Insert," Diamond and Related Materials, 2 (1993) pp. 1391-1395.
Haubner et al., "Diamond Growth by Hot-Filament Chemical Vapor Deposition: State of the Art," Diamond and Related Materials, 2 (1993) pp. 1277-1294.
Yarbrough et al., "The Chemical Vapor Deposition of Diamond," Materials Science Forum, vols. 52 and 53 (1989) pp. 151-174.
Saijo et al., "The Improvement of the Adhesion Strength of Diamond Films," Surface and Coatings Technology, 43/44 (1990) pp. 30-40.
Lux et al., "Low Pressure Synthesis of Superhard Coatings," Int. J. Ref. & Hard Mater., 8 (1989) pp. 158-174.
Kuo et al., "Adhesion and Tribological Properties of Diamond Films on Various Substrates," J. Mater. Res., vol. 5, No. 11, Nov. 1990, pp. 2515-2523.
Kikuchi et al., "Diamond Coated Inserts: Characteristics and Performance," Applications of Diamond Films and Related Materials, Ed. by Tzeng et al., (1991) pp. 61-68.
McCune et al., "An Auger Electron Spectroscopy Study of the Surface of Ni-Mo Cemented Ti(CN) Substrates Used for Deposition of Crystalline Diamond Particles," Surface & Coatings Technology, 39/40 (1989) pp. 223-233.
Jindal et al., "Adhesion Measurements of Chemically Vapor Deposited & Physically Vapor Deposited Hard Coatings on WC-Co Substrates," Thin Solid Films, 154 (1987) pp. 361-375.
"Metals Handbook Ninth Edition," vol. 7, Powder Metallurgy (1984) pp. 385-388, 398.
Soderberg et al., "Factors Influencing the Adhesion of Diamond Coatings on Cutting Tools," Vacuum, vol. 41, No. 4-6, (1990) pp. 1317-1321.
Murakawa et al., "Chemical Vapour Deposition of a Diamond Coating onto a Tungsten Carbide Tool Using Ethanol," Surface and Coatings Technology, 36 (1988) pp. 303-310.
Park et al., "Behaviour of Co Binder Phase during Diamond Deposition on WC-Co Substrate," Diamond and Related Materials, 2 (1993) pp. 910-917.
Saito et al., "Application of Diamond Films from CO-H.sub.2 Plasma to Tool Blade Coating," Journal of Materials Science, 26, (1991) pp. 2937-2940.
Nesladek et al., "Improved Adhesion of CVD Diamond Films to Steel and WC-Co Substrates," Diamond and Related Materials, 3 (1993) pp. 98-104.
JIS B 0601 (1982) "Definitions and Designation of Surface Roughness," JIS Handbook 1989 Tools, Japanese Standards Association (1989) pp. 2245-2255.
"Surface Texture and Roundness Measurement Handbook," Sheffield Measurement Division, Warner & Swasey (1988) pp. 47, 48.
Tulhoff, "On the Grain Growth of WC in Cemented Carbides," Modern Developments in Powder Metallurgy, ed. by Hausner et al., vol. 14, Special Materials (1981) pp. 269-279.
Rudiger et al., "On the Problem of Evaporation of the Auxiliary Metal During Vacuum Sintering of Hard Metals," Int'l. Symp. on Powder Met., Paris, Jun. 1964, pp. 259-269.
Gaser, "Edge and Surface Honing on Various Shaped PCD & CBN Inserts," SME Technical Paper MR92-357 (1992).
Scheider, "Edge Grinding and Radiusing with Superabrasives," MAN, Sep. 1992, pp. 46-47.
Hosomi et al., "Diamond CVD Researchers as Patent Applied," Applications of Diamond Films and Related Materials, ed. by Tzeng et al., Proceedings of Auburn University Conference, Aug. 1991, Elsevier Science Publishers B.V., (1991) pp. 15-24.
Israelsson, "A Progress Report on Cutting Tool Materials," American Machinist, Dec. 1992, pp. 39, 40.
"Advanced Cutting Tool Materials," Kennametal Catalogue No. A90-67 (1988) pp. 1, 2, 77-86, 94-98, 101 and 102.
"Standard Test Method for Apparent Porosity in Cemented Carbides," ASTM Designation: B276-86. No date and year available.
"American National Standard for Cutting Tools--Indexable Inserts--Identification System" ANSI B212,Apr. 1986.
Eastman et al., "Machining MMCs," Cutting Tool Engineering, Oct. 1993, pp. 38, 40-44.
Scheider, "Precision Edge Radius Grinding of Diamond Cutting Tools and Inserts," SME Technical Paper MR91-195 (1991).
Scheider, "New Abrasive Edge and Surface Preparation Tools, Techniques and Technology for Fabricated Material Applications," SME Technical Paper FC91-426 (1991).
Bauer Charles Erik
Grab George P.
Inspektor Aharon
Melago William M.
Murray Gerald D.
Kennametal Inc.
King Roy V.
Prizzi John J.
LandOfFree
Process for making diamond coated tools and wear parts does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for making diamond coated tools and wear parts, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for making diamond coated tools and wear parts will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1491096