Process for converting water sensitive ceramic powders into a fr

Plastic and nonmetallic article shaping or treating: processes – Pore forming in situ – By mechanically introducing gas into material

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

264 6, 264 7, 264 12, 264 61, 264 63, C04B 35622, B29B 900

Patent

active

054983827

ABSTRACT:
A water sensitive ceramic powder, in particular aluminum nitride, is provided with a hydrophobic coating. The coated powder is dispersed in water with addition of a binder and a nonionic surfactant from the group comprising ethylene oxide adducts with an HLB value of from 10 to 14. Subsequently the aqueous slip is converted into a free flowing granulated powder. The nonionic surfactant, which is added in an amount sufficient to give a monomolecular layer, makes possible a good dispersion of the hydrophobically coated powder in water.

REFERENCES:
patent: 4401366 (1983-08-01), Hope
patent: 4978465 (1990-12-01), Sturwold
patent: 5175051 (1992-12-01), Schloegl et al.
patent: 5182239 (1993-01-01), Hirokawa et al.
patent: 5288806 (1994-02-01), Peacock
Chemical Abstracts, vol. 11, No. 6, Aug. 7, 1989, abstract No. 44266f, Nakamura "Free Flowing granulated aluminum nitride powder for press molding" & JP-A-1061632, Mar. 8, 1989.
Database WPI, Section CH, Week 8928, Derwent Publications Ltd. Class A81, AN 89-203080 & JP-A-1 141 865 (Mitsubishi Mining Cement) Jun. 2, 1989.
Database WPI, Section CH, Week 8916, Derwent Publications Ltd., Class E33, AN 89-117143, & JP-A-1061304 (Denki Kagaku Kogyo KK) Mar. 8, 1989.
Chemical Abstracts, vol. 108, No. 8, Feb. 22, 1988, Columbus, Ohio, Abstract No. 61239e, Uno Naoki & Al. "Surface treatment of aluminum nitride powder . . . ", JP-A-62207770, Sep. 12, 1987.
Patent Abstracts of Japan, vol. 013, No. 021 (C-560), Jan. 18, 1989 & JP-A-63 225 507 Sep. 1988.
Database Inspec, Institute of Electrical Engineers, No. 4014683, Egashira et al. "Chemical surface treatments of aluminum nitride powder suppressing its reactivity with water . . . ".
Von R. Heusch, Eine experimentelle Methode zur Bestimmung des HLB-Wertes von Tensiden; Jul. 7, 1969 pp. 31-38.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for converting water sensitive ceramic powders into a fr does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for converting water sensitive ceramic powders into a fr, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for converting water sensitive ceramic powders into a fr will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2098503

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.