ABSTRACT:
Polymer buildup in polymerization reactions during vinyl chloride polymerizations is greatly reduced by applying a water dispersion of alumina and oxalyl bis(benzylidenehydrazide) (OABH) to the reactor surfaces exposed to the polymerization medium prior to carrying out the polymerization. Long term effects of the buildup preventor can be obtained by applying a caustic wash to the reactor walls, prior to applying the oxalyl bis(benzylidenehydrazide) and alumina dispersion. The effect of the OABH/alumina and caustic is synergistic since the preventative effect is greater than either material used alone.
REFERENCES:
patent: 4068052 (1978-01-01), Weimer et al.
Freshour Kenneth D.
Weimer Dean R.
Continental Oil Company
Kight III John
Schupbach, Jr. Cortlan R.
LandOfFree
Prevention of PVC polymer buildup in polymerization reactors usi does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Prevention of PVC polymer buildup in polymerization reactors usi, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Prevention of PVC polymer buildup in polymerization reactors usi will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-221747