ABSTRACT:
Nickel based superalloys with excellent mechanical strength, corrosion resistance and oxidation resistance, which consist essentially of chromium in an amount of 3 to 7% by weight, cobalt in an amount of 3 to 15% by weight, tungsten in an amount of 4.5 to 8% by weight, rhenium in an amount of 3.3 to 6% by weight, tantalum in an amount of 4 to 8% by weight, titanium in an amount of 0.8 to 2% by weight, aluminum in an amount of 4.5 to 6.5% by weight, ruthenium in an amount of 0.1 to 6%, hafnium in an amount of 0.01 to 0.2% by weight, molybdenum in an amount of less than 0.5% by weight, carbon in an amount 0.06% by weight or less, boron in an amount of 0.01% by weight or less, zirconium in an amount of 0.01% by weight or less, oxygen in an amount of 0.005% by weight or less, nitrogen in an amount of 0.005% by weight or less and inevitable impurities and the balance being nickel.

REFERENCES:
patent: 4935072 (1990-06-01), Nguyen-Dinh
patent: 5151249 (1992-09-01), Austin et al.
patent: 5366695 (1994-11-01), Erickson
patent: 5455120 (1995-10-01), Walston et al.
patent: 5482789 (1996-01-01), O'Hara et al.
patent: 6007645 (1999-12-01), Cetel et al.
patent: 6444057 (2002-09-01), Darolia et al.
patent: 6648596 (2003-11-01), Grylls et al.
patent: 7115175 (2006-10-01), DeLuca et al.
patent: 2002/0172808 (2002-11-01), Wustman et al.
patent: 2007/0163682 (2007-07-01), Tamaki et al.
patent: 0663462 (1995-07-01), None
patent: 10-195565 (1998-07-01), None
Zheng et al., “Effect of RU Addition on Cast Nickel Base Superalloy with Low Content of CR and High Content of W” Superalloys 2000, pp. 305-311, The Minerals, Metals & Materials Society.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Nickel based superalloys with excellent mechanical strength,... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Nickel based superalloys with excellent mechanical strength,..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Nickel based superalloys with excellent mechanical strength,... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-4059490

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.