ABSTRACT:
A continuous annealing process for producing a soft tin plate and black plate with T - 21/2 or T - 3 tempering properties is attained in a conventional continuous annealing furnace for black plate by the use of a novel steel strip composition.

REFERENCES:
patent: 3806376 (1974-04-01), Toda et al.
patent: 3839095 (1974-10-01), Kubotera et al.
patent: 3920487 (1975-11-01), Gondo et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of producing soft thin steel sheet by continuous annealin does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of producing soft thin steel sheet by continuous annealin, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of producing soft thin steel sheet by continuous annealin will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1832856

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.