Synthetic resins or natural rubbers -- part of the class 520 ser – Synthetic resins – Treating polymer containing material or treating a solid...
Patent
1996-12-18
2000-10-17
Henderson, Christopher
Synthetic resins or natural rubbers -- part of the class 520 ser
Synthetic resins
Treating polymer containing material or treating a solid...
523307, C08C 1908
Patent
active
061334138
ABSTRACT:
Devulcanized rubber in which sulfuric crosslinking bonds are cut and which contains carbon black particles having very small diameters. Vulcanized rubber of discarded products is devulcanized by heating it at a temperature of 180.degree. C. --350.degree. C. and applying a shearing pressure of 10-150 kg/cm.sup.2 thereto. Reclaimed rubber products are manufactured by vulcanizing and molding, into desired shapes, a material made of only devulcanized rubber in which sulfuric crosslinking bonds are cut and which contains carbon black particles having very small diameters or a material made of the devulcanized rubber mixed with virgin unvulcanized rubber.
REFERENCES:
patent: 2461192 (1949-02-01), Banbury
Honda Hidenobu
Ichikawa Masayoshi
Mouri Makoto
Murase Atsushi
Nakashima Katsumi
Henderson Christopher
Kabushiki Kaisha Toyota Chuo Kenkyusho
Toyoda Gosei Co,., Ltd.
Toyota Jidosha & Kabushiki Kaisha
LandOfFree
Method of manufacturing devulcanized rubber using high temperatu does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of manufacturing devulcanized rubber using high temperatu, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of manufacturing devulcanized rubber using high temperatu will most certainly appreciate the feedback.