ABSTRACT:
Glass laser rods are treated and strengthened by a method which produces a ardened surface that protects the laser rods from physical abrasion, prevents failure due to thermal shock, and removes flaws while not interfering with light pumping through the sides of the treated rods. The method includes subjecting the prepared glass laser rods to an acid polishing procedure which employs an acid polishing solution comprised of equal parts of concentrated hydrofluoric and concentrated nitric acid.

REFERENCES:
patent: 3023139 (1962-02-01), Van Tetterupe
patent: 3171768 (1963-03-01), Levengood
patent: 3301649 (1967-11-01), Marusak
patent: 3647583 (1972-03-01), De Rouw
patent: 3687799 (1972-08-01), Spanoudis
patent: 3779732 (1973-12-01), Spanoudis
patent: 3843472 (1974-10-01), Toussaint et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of increasing the strength of silicate glass laser rods does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of increasing the strength of silicate glass laser rods, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of increasing the strength of silicate glass laser rods will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2078668

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.