ABSTRACT:
A process for producing a slightly Cu-poor thin film of Cu(In,Ga)(Se,S).sub.2 comprises depositing a first layer of (In,Ga).sub.x (Se,S).sub.y followed by depositing just enough Cu+(Se,S) or Cu.sub.x (Se,S) to produce the desired slightly Cu-poor material. In a variation, most, but not all, (about 90 to 99%) of the (In,Ga).sub.x (Se,S).sub.y is deposited first, followed by deposition of all the Cu+(Se,S) or Cu.sub.x (Se,S) to go near stoichiometric, possibly or even preferably slightly Cu-rich, and then in turn followed by deposition of the remainder (about 1 to 10%) of the (In,Ga).sub.x (Se,S).sub.y to end with a slightly Cu-poor composition. In yet another variation, a small portion (about 1 to 10%) of the (In,Ga).sub.x (Se,S).sub.y is first deposited as a seed layer, followed by deposition of all of the Cu+(Se,S) or Cu.sub.x (Se,S) to make a very Cu-rich mixture, and then followed deposition of the remainder of the (In,Ga).sub.x (Se,S).sub.y to go slightly Cu-poor in the final Cu(In,Ga)(Se,S).sub.2 thin film.
REFERENCES:
patent: 4465574 (1984-08-01), Love et al.
patent: 4652332 (1987-03-01), Ciszek
patent: 4684761 (1987-08-01), Devaney
patent: 4798660 (1989-01-01), Ermer et al.
patent: 4818357 (1989-04-01), Case et al.
patent: 4915745 (1990-04-01), Pollock et al.
patent: 5045409 (1991-09-01), Eberspacher et al.
patent: 5141564 (1992-08-01), Chen et al.
patent: 5356839 (1994-10-01), Tuttle et al.
Albin David S.
Carapella Jeffrey J.
Contreras Miguel A.
Gabor Andrew M.
Noufi Rommel
Midwest Research Institute
O'Connor Edna M.
Weisstuch Aaron
LandOfFree
Method of fabricating high-efficiency Cu(In,Ga)(SeS).sub.2 thin does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of fabricating high-efficiency Cu(In,Ga)(SeS).sub.2 thin , we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of fabricating high-efficiency Cu(In,Ga)(SeS).sub.2 thin will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2181317