ABSTRACT:
Stress corrosion cracking 36 at a welded pipe joint 14 in service in a nuclear reactor can be controlled by the location of a overlay weld 18 over the primary weld 16, which extends axially along the pipe on either side of the primary weld 16. The overlay weld 18 is comprised of a plurality of circumferentially and continuously applied weld beads 35, 37 which extend substantially to a minimum distance necessary to produced a favorable residual stress pattern. This distance has been estimated to be the square root of the product of the radius of the pipe times the thickness of the pipe on either side of the primary weld 16.

REFERENCES:
patent: 2963129 (1960-12-01), Eberle
patent: 4049186 (1977-09-01), Hanneman et al.
patent: 4348041 (1982-09-01), Imai et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for applying an overlay weld for preventing and controlli does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for applying an overlay weld for preventing and controlli, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for applying an overlay weld for preventing and controlli will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1154538

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.