ABSTRACT:
A process for the manufacture of an acicular magnetic iron oxide containing from 0.5 to 10 percent by weight of cobalt and up to 24 percent by weight of divalent iron, each based on the amount of iron(III) oxide, wherein an aqueous suspension of gamma-iron(III) oxide, containing cobalt(II) and iron(II) ions, the suspension having a hydroxyl ion concentration of more than 3.6.times.10.sup.-6 moles/liter, is heated at from 50.degree. to 100.degree. C. for at least 15 minutes, and the resulting precipitate is filtered off, washed until neutral, dried at below 100.degree. C. and thereafter heated at from 100.degree. to 200.degree. C.
The products thus obtained give, even when their cobalt content is low, a very high coercive force, while the effect of temperature on the coercive force and residual induction is very slight.

REFERENCES:
patent: 4015030 (1977-03-01), Sasazawa et al.
patent: 4066564 (1978-01-01), Sasazawa et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Manufacture of acicular cobalt-modified magnetic iron oxide does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Manufacture of acicular cobalt-modified magnetic iron oxide, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Manufacture of acicular cobalt-modified magnetic iron oxide will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1854357

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.