Irregular shape change of tungsten/matrix interface in tungsten

Powder metallurgy processes – Powder metallurgy processes with heating or sintering – Post sintering operation

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

419 58, B22F 324

Patent

active

059565594

ABSTRACT:
A method for producing an irregular tungsten/matrix interface in tungsten based heavy alloy is disclosed. The method involves a cyclic heat treatment and resintering at above liquidus temperature for tungsten heavy alloys consisting of 80 to 98 weight % tungsten and remainder of matrix phase. The sintered specimens are cyclically heat treated at above 1000.degree. C. and resintered at liquidus temperature of the matrix phase for one minute to 4 hours at a constant temperature.

REFERENCES:
patent: 3307982 (1967-03-01), Milligan et al.
patent: 3979234 (1976-09-01), Northcutt, Jr. et al.
patent: 3988118 (1976-10-01), Grierson et al.
patent: 4002471 (1977-01-01), Sarnes et al.
patent: 4762559 (1988-08-01), Penrice et al.
patent: 4784690 (1988-11-01), Mullendore
patent: 4938799 (1990-07-01), Nicolas
patent: 5145512 (1992-09-01), Spencer et al.
patent: 5248474 (1993-09-01), Morgan
patent: 5294269 (1994-03-01), Lee et al.
patent: 5342573 (1994-08-01), Amano et al.
patent: 5462516 (1995-10-01), Stuitje et al.
patent: 5722034 (1998-02-01), Kambara
Heung-Sub Song, et al., "Undulation of W/Matrix Interface by Resintering of Cyclically Heat-Treated W-Ni-Fe Heavy Alloys", Metallurgical and Materials Transactions A, vol. 28A, pp. 485-489 (Feb. 1997).

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Irregular shape change of tungsten/matrix interface in tungsten does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Irregular shape change of tungsten/matrix interface in tungsten , we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Irregular shape change of tungsten/matrix interface in tungsten will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-90641

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.