ABSTRACT:
Integrated circuits and methods of redistributing bondpad locations are disclosed. In one implementation, a method of redistributing a bondpad location of an integrated circuit includes providing an integrated circuit comprising an inner lead bondpad. A first insulative passivation layer is formed over the integrated circuit. A bondpad-redistribution line is formed over the first insulative passivation layer and in electrical connection with the inner lead bondpad through the first insulative passivation layer. The bondpad-redistribution line includes an outer lead bondpad area. A second insulative passivation layer is formed over the integrated circuit and the bondpad-redistribution line. The second insulative passivation layer is formed to have a sidewall outline at least a portion of which is proximate to and conforms to at least a portion of the bondpad-redistribution line. Other aspects and implementations are contemplated.
REFERENCES:
patent: 6551856 (2003-04-01), Lee
patent: 6664176 (2003-12-01), Hedler et al.
patent: 7262121 (2007-08-01), Watkins
patent: 2003/0098513 (2003-05-01), Huang
patent: 2004/0032013 (2004-02-01), Cobbley et al.
patent: 2004/0033673 (2004-02-01), Cobbley et al.
patent: 2004/0036137 (2004-02-01), Gleason et al.
patent: 2004/0040855 (2004-03-01), Batinovich
patent: 2004/0195687 (2004-10-01), Inoue et al.
patent: 2006/0022350 (2006-02-01), Watkins
patent: 2006/0214309 (2006-09-01), Watkins
patent: 2006/0223298 (2006-10-01), Watkins
patent: 2007/0194458 (2007-08-01), Watkins
patent: 2008/0006931 (2008-01-01), Oliver et al.
patent: 2008/0036067 (2008-02-01), Lin
patent: 2008/0061411 (2008-03-01), Shen et al.
patent: 2008/0061412 (2008-03-01), Shen et al.
patent: 2008/0061421 (2008-03-01), Shen et al.
patent: 2008/0099892 (2008-05-01), Chen et al.
patent: 2008/0099896 (2008-05-01), Shen et al.
Blakenhorn et al.,A Semi-Additive Electroless Ni/Au Process Offers a Low-Cost Wafer-Bumping Method, Chip Scale Review Online, 9 pages (Jul. 2001).
Menz Laura M
Micro)n Technology, Inc.
Wells St. John P.S.
LandOfFree
Integrated circuit and methods of redistributing bondpad... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Integrated circuit and methods of redistributing bondpad..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Integrated circuit and methods of redistributing bondpad... will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-4003546