ABSTRACT:
In the deinking of feed waste papers comprising magazines and newspapers at a weight ratio of magazine to newspaper of from 5/95 to 60/40, a reclaimed pulp with excellent qualities can be obtained by adjusting the treating temperature in the flotation step to 40.degree. to 80.degree. C. and adding a deinking agent, which contains an alkylene oxide adduct of an oil or fat, wherein said alkylene oxide adduct comprises ethylene oxide and propylene oxide added at a molar ratio of ethylene oxide to propylene oxide of from 1/1 to 5/1, and has a cloud point of 45.degree. to 90.degree. C., at least in one of the steps of the deinking process.
REFERENCES:
patent: 5100574 (1992-03-01), Urushibata et al.
patent: 5221433 (1993-06-01), Daute et al.
patent: 5281358 (1994-01-01), Urushibata et al.
patent: 5304316 (1994-04-01), Urushibata et al.
Hamaguchi Koji
Takahashi Hiromichi
Czaja Donald E.
Kao Corporation
Leavitt Steven B.
LandOfFree
High temperature deinking method using an alkylene oxide adduct does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with High temperature deinking method using an alkylene oxide adduct, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and High temperature deinking method using an alkylene oxide adduct will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2254420