ABSTRACT:
AlPO.sub.4 crystals are isomorphic with quartz and are expected therefore to have several crystal orientations in which the elastic (piezoelectric) constants are relatively insensitive to temperature. The piezoelectric coupling coefficients of AlPO.sub.4 are approximately three times those of quartz. Hydrothermal growth techniques to date have been marginal, and all have employed H.sub.3 PO.sub.4 as the hydrothermal solution. We describe using HCl as the hydrothermal solution and demonstrate the superiority of HCl from the standpoint of solubility and consequent crystal growth rate.
REFERENCES:
patent: 3567643 (1971-03-01), Flanigen et al.
patent: 3634044 (1972-01-01), Parker
patent: 3723337 (1973-03-01), Yancy
patent: 4247358 (1981-01-01), Aucoin et al.
Pamplin, Crystal Growth, Second Edition, vol. 16, Permagon Press (1980), pp. 464-466.
Kolb Ernest D.
Laudise Robert A.
Bell Telephone Laboratories Incorporated
Langel Wayne A.
Vertiz O. R.
Wilde Peter V. D.
LandOfFree
Growth of AlPO.sub.4 crystals does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Growth of AlPO.sub.4 crystals, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Growth of AlPO.sub.4 crystals will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1291200