Compositions: ceramic – Ceramic compositions – Refractory
Patent
1991-03-13
1994-01-04
Lesmes, George F.
Compositions: ceramic
Ceramic compositions
Refractory
428367, 428368, 428378, 428380, 428384, 428902, B32B 1800, C04B 3571
Patent
active
052759849
ABSTRACT:
A composite comprising a ceramic matrix having immersed ceramic reinforcing fibers is strengthened and toughened by providing a multi-layer ceramic coating surrounding each fiber. The multiple layers in the fiber coating are not bonded to one another. As a result, the multiple layers separate from one another in the presence of an advancing crack in the ceramic matrix, thereby permitting the fibers to pull out of the matrix and avoid premature fiber breakage. The choice of materials for the fiber coating is not limited by any requirement to establish a particular type of chemical bond between the coating and the fiber. Instead, the invention relies only upon the mechanical tendency of the unbonded multiple layers in the fiber coating to separate to promote fiber pull-out from the matrix in the wake of an advancing crack.
REFERENCES:
patent: 4405685 (1983-09-01), Honjo et al.
patent: 4732877 (1988-03-01), Olson et al.
patent: 4772524 (1988-09-01), Coblenz
patent: 4837230 (1989-06-01), Chen et al.
patent: 4863798 (1989-09-01), Arenz et al.
patent: 4867761 (1989-09-01), Brandt et al.
patent: 4885199 (1989-12-01), Corbin et al.
patent: 4919991 (1990-04-01), Gadkaree
patent: 4935387 (1990-06-01), Beall et al.
patent: 5017528 (1991-05-01), Tiegs et al.
patent: 5026604 (1991-06-01), Thebault
patent: 5057465 (1991-10-01), Sakamoto et al.
patent: 5134020 (1992-07-01), Cotteret et al.
Bohlen James W.
Carpenter Harry W.
Anderson Terry J.
Block Robert B.
Brown Christopher
Hoch Jr. Karl J.
Lesmes George F.
LandOfFree
Fiber coating of unbonded multi-layers for toughening ceramic fi does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Fiber coating of unbonded multi-layers for toughening ceramic fi, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Fiber coating of unbonded multi-layers for toughening ceramic fi will most certainly appreciate the feedback.