Alloys or metallic compositions – Nickel base – Chromium containing
Patent
1990-08-01
1992-07-14
Dean, R.
Alloys or metallic compositions
Nickel base
Chromium containing
148434, C22C 1905
Patent
active
051300869
ABSTRACT:
The present invention provides an alloy having improved crack growth inhibition and having high strength at high temperatures. The composition of the alloy is essentially as follows:
REFERENCES:
patent: 3061426 (1962-10-01), Bieber
patent: 3589893 (1971-06-01), Lund et al.
patent: 3825420 (1974-07-01), Ewing et al.
patent: 3902862 (1975-09-01), Moll et al.
patent: 4207098 (1980-06-01), Shaw
G. W. Meetham, "Development of Gas Turbine Materials", Applied Science Publishers, London, Great Britian (1981) pp. 296-298.
Davis Jr. James C.
Dean R.
General Electric Company
Magee Jr. James
Phipps Margery S.
LandOfFree
Fatigue crack resistant nickel base superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Fatigue crack resistant nickel base superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Fatigue crack resistant nickel base superalloys will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-333222