Fatigue crack-resistant nickel base superalloy composition

Alloys or metallic compositions – Nickel base – Chromium containing

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

148410, 148428, 420588, C22C 1905

Patent

active

051568080

ABSTRACT:
The present invention provides an alloy having improved crack growth inhibition and having high strength at high temperatures. The composition of the alloy is essentially as follows:

REFERENCES:
patent: 3061426 (1962-10-01), Bieber
patent: 3589893 (1971-06-01), Lund et al.
patent: 3677747 (1972-07-01), Lund et al.
patent: 3825420 (1974-07-01), Ewing et al.
patent: 3869284 (1975-03-01), Baldwin
patent: 4207098 (1980-06-01), Shaw
patent: 4853044 (1989-08-01), Ford et al.
G. W. Meetham, "Development of Gas Turbine Materials", Applied Science Publishers, London, Great Britain (1981) pp. 296-298.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Fatigue crack-resistant nickel base superalloy composition does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Fatigue crack-resistant nickel base superalloy composition, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Fatigue crack-resistant nickel base superalloy composition will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-190457

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.