Alloys or metallic compositions – Nickel base – Chromium containing
Patent
1990-09-04
1992-10-20
Andrews, Melvyn J.
Alloys or metallic compositions
Nickel base
Chromium containing
148410, 148428, 420588, C22C 1905
Patent
active
051568080
ABSTRACT:
The present invention provides an alloy having improved crack growth inhibition and having high strength at high temperatures. The composition of the alloy is essentially as follows:
REFERENCES:
patent: 3061426 (1962-10-01), Bieber
patent: 3589893 (1971-06-01), Lund et al.
patent: 3677747 (1972-07-01), Lund et al.
patent: 3825420 (1974-07-01), Ewing et al.
patent: 3869284 (1975-03-01), Baldwin
patent: 4207098 (1980-06-01), Shaw
patent: 4853044 (1989-08-01), Ford et al.
G. W. Meetham, "Development of Gas Turbine Materials", Applied Science Publishers, London, Great Britain (1981) pp. 296-298.
Andrews Melvyn J.
Davis Jr. James C.
General Electric Company
Phipps Margery S.
Pittman William H.
LandOfFree
Fatigue crack-resistant nickel base superalloy composition does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Fatigue crack-resistant nickel base superalloy composition, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Fatigue crack-resistant nickel base superalloy composition will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-190457