ABSTRACT:
A method for hot-dip coating a steel strip comprises: (a) continuously annealing the steel strip in an annealing furnace; (b) introducing the annealed steel strip into a molten metal coating bath through a snout; (c) dipping the annealed steel strip into the molten metal coating bath; (d) controlling a pressure inside of the snout; and (e) discharging a gas containing a metal vapor from the snout to outside of the snout. An apparatus comprises an annealing furnace, a coating pot, a control device for controlling a pressure inside the snout and a gas discharging device.
REFERENCES:
patent: 4107357 (1978-08-01), Asakawa et al.
patent: 4439212 (1984-03-01), Wang
patent: 4466999 (1984-08-01), Leonard
patent: 4478892 (1984-10-01), Amberson
patent: 5339329 (1994-08-01), Flinchum et al.
Akashi Kentaro
Fukui Takayuki
Hatakeyama Seishi
Hiraya Akira
Ishida Nobuyuki
Barr Michael
King Roy V.
NKK Corporation
LandOfFree
Continuous hot-dip coating method and apparatus therefor does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Continuous hot-dip coating method and apparatus therefor, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Continuous hot-dip coating method and apparatus therefor will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1334989