Plastic and nonmetallic article shaping or treating: processes – Outside of mold sintering or vitrifying of shaped inorganic... – Involving specified composition of heating atmosphere – other...
Reexamination Certificate
2006-06-27
2006-06-27
Vincent, Sean (Department: 1731)
Plastic and nonmetallic article shaping or treating: processes
Outside of mold sintering or vitrifying of shaped inorganic...
Involving specified composition of heating atmosphere, other...
C501S065000, C501S055000, C501S118000
Reexamination Certificate
active
07067085
ABSTRACT:
This invention provides a black low thermal expansion high specific rigidity ceramic sintered body having a black tone, manifesting very small thermal expansion at room temperature and abounding in rigidity and specific rigidity, and a method for the production thereof. The black low thermal expansion high specific rigidity ceramic sintered body is characterized by having a chemical composition comprising 8.0–17.2 mass % of MgO, 22.0–38.0 mass % of Al2O3, 49.5–65.0 mass % of SiO2, a total of 0.1–2 mass % of one or more transition elements as reduced to oxides, and 0–2.5 mass % of Li2O, and having the mass ratios satisfy the relationships of (SiO2−8×Li2O)/MgO≧3.0 and (SiO2−8×Li2O)/Al2O3≧1.2. The method for the production of a black low thermal expansion high specific rigidity ceramic sintered body of this invention is characterized by forming the sintered body in an atmosphere of a non-oxidizing gas at a temperature in the range of 1200–1500° C.
REFERENCES:
patent: 6265334 (2001-07-01), Sechi et al.
patent: 6372677 (2002-04-01), Nose et al.
patent: 198 49 340 (1999-04-01), None
patent: 1 094 046 (2001-04-01), None
patent: 57-38371 (1982-03-01), None
patent: 57-29436 (1982-06-01), None
patent: 61-72679 (1986-04-01), None
patent: 63-210060 (1988-08-01), None
patent: 402074538 (1990-03-01), None
patent: 403150263 (1991-06-01), None
patent: 4-50161 (1992-02-01), None
patent: 6-172034 (1994-06-01), None
patent: 8-310860 (1996-11-01), None
patent: 10-53460 (1998-02-01), None
patent: 11-343168 (1999-12-01), None
patent: 2000-290064 (2000-10-01), None
patent: P3133302 (2000-11-01), None
Collected Catalogs of Fine Ceramics, “Low Thermal Expansion Ceramics”, Japan Fine Ceramics Society, 1987, p. 140, and English translation.
Ceramics, vol. 18 (1983) No. 5, “Ceramic Pigments”, p. 377, by A. Ohtsuka, and partial English translation.
Data Base WPI Abstract of Japan No. 61-178038 published Aug. 9, 1986.
Hashimoto Katsumi
Morita Hidehiko
Nose Tetsuro
Sugawara Jun
Kenyon & Kenyon LLP
Lopez Carlos
Nippon Steel Corporation
Vincent Sean
LandOfFree
Black ceramic sinter with low thermal expansion and high... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Black ceramic sinter with low thermal expansion and high..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Black ceramic sinter with low thermal expansion and high... will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-3700258