ABSTRACT:
High temperature oxidation resistance of an aluminide diffusion overcoated MCrAlY coating system is substantially improved by CVD over-aluminizing the MCrAlY type overlay coating under CVD conditions that result in reduced concentrations of such tramp impurities as S and P in the aluminized MCrAlY overlay coating region of the coating system. The CVD aluminizing conditions yield an outwardly grown aluminide over-coat on the underlying MCrAlY type coating.
REFERENCES:
patent: 4080486 (1978-03-01), Walker et al.
patent: 5658614 (1997-08-01), Basta et al.
patent: 5716720 (1998-02-01), Murphy
patent: 5763107 (1998-06-01), Rickerby et al.
patent: 5788823 (1998-08-01), Warnes et al.
Evaluation of Simple Aluminide and Platinum Modified Aluminide Coatings on High Pressure Turbine Blades after Factory Engine Testing--Round II International Gas Turbine and Aeroengine Congress and Exposition, Jun. 1-4, 1992, Conner.
Platinum Modified Aluminides--Present Status, Gas Turbine and Aeroengine Congress and Exposition, Jun. 11-14, 1990, Smith et al.
Evaluation of Simple Aluminide and Platinum Modified Aluminide Coatings on High Pressure Turbine Blades after Factory Engine Testing International Gas Turbine and Aeroengine Congress and Exhibition, Jun. 3-6, 1991, Conner et al.
DuShane Nick S.
Honick, Jr. Ronald J.
Shriver William J.
Warnes Bruce M.
Howmet Research Corporation
Speer Timothy M.
Timmer Edward J.
Young Bryant
LandOfFree
Aluminide/MCrAlY coating system for superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Aluminide/MCrAlY coating system for superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Aluminide/MCrAlY coating system for superalloys will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2254772