ABSTRACT:
A process of producing 99% plus titanium dioxide product by using conventional and microwave heating and leaching of the titanium compound feedstock using acid and oxidants. The solid residue from the leaching is used to produce the high quality titanium oxide by froth flotation. Hydrochloric acid can be recovered by multi-stage evaporation. The process can be modified to produce nano-size titanium dioxide product.

REFERENCES:
patent: 3457037 (1969-07-01), Aramendia et al.
patent: 3803287 (1974-04-01), Fukushima et al.
patent: 3922164 (1975-11-01), Reid et al.
patent: 4097574 (1978-06-01), Auger et al.
patent: WO96/24555 (1996-08-01), None

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Acid/microwave leaching of titanium ore and then flotation... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Acid/microwave leaching of titanium ore and then flotation..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Acid/microwave leaching of titanium ore and then flotation... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-4109538

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.