Process for forming tin oxide conductive pattern

Adhesive bonding and miscellaneous chemical manufacture – Delaminating processes adapted for specified product – Delaminating in preparation for post processing recycling step

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

156651, 1566591, 1566611, 156901, 427 66, 427110, 4271262, 4271263, 428 1, C03C 1710

Patent

active

043448178

ABSTRACT:
A pattern of transparent conductive material, such as tin oxide, is formed on a transparent vitreous substrate using a polycrystalline material, such as cadmium or zinc sulfide, to mask the substrate surface while depositing material forming the transparent conductive layer. The polycrystalline material and any overlying transparent conductive material are easily removed by a chemical etch, leaving the desired pattern of transparent conductive material adhering to the substrate. Two electrically conductive patterns may be formed in intersecting relationship and isolated, one from the other. The degree of electrical connection between the two patterns will be a function of the resistance of the polycrystalline material therebetween at points of crossing. In some instances, electroluminescence may be obtained by selecting the proper crystalline material wherein an electrical display may be created by selectively energizing crossing electrical conductors.

REFERENCES:
patent: 2850409 (1958-09-01), Boicey et al.
patent: 2919366 (1959-12-01), Mash
patent: 3003904 (1961-10-01), Riggen
patent: 3423260 (1969-01-01), Heath et al.
patent: 3588570 (1961-06-01), O'Keeffe
patent: 3647566 (1972-03-01), Szupillo
patent: 3669770 (1972-06-01), Fedlstein
patent: 3874916 (1975-04-01), Livesay et al.
patent: 3880633 (1975-04-01), Jordan et al.
patent: 3922420 (1975-11-01), Schnable et al.
patent: 3928658 (1975-12-01), Van Boxtel et al.
patent: 3959565 (1976-05-01), Jordan et al.
patent: 3991227 (1976-11-01), Carlson et al.
patent: 4009061 (1977-02-01), Simon
patent: 4018938 (1977-04-01), Feder et al.
patent: 4059069 (1977-11-01), Ford
patent: 4095006 (1978-06-01), Jordan et al.
patent: 4119245 (1978-10-01), Smith
patent: 4158072 (1979-06-01), Bohg et al.
patent: 4178403 (1979-12-01), Sakurai et al.
patent: 4224355 (1978-03-01), Lampkin et al.
patent: 4239809 (1980-12-01), Lampkin et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for forming tin oxide conductive pattern does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for forming tin oxide conductive pattern, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for forming tin oxide conductive pattern will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-185799

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.