ABSTRACT:
A cationically-conductive polycrystalline body having a specific resistivity at its surface portion higher than its specific intrinsic resistivity is contacted with phosphoric acid to produce an etched body having a uniform specific intrinsic resistivity.

REFERENCES:
patent: 3964942 (1976-06-01), Berkenblit et al.
patent: 4141781 (1979-02-01), Greskovich et al.
Mat. Res. Bull., vol. 5, No. 3, pp. 167-171, 1970, Pergamon Press, Inc., printed in the U.S., The Chemical Polishing of Magnesium Aluminate Spinel in Pyrophosphoric Acid, R. Aeschlimann et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of etching to form cationically-conductive ceramic body does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of etching to form cationically-conductive ceramic body, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of etching to form cationically-conductive ceramic body will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1563762

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.