ABSTRACT:
Boron nitride, in its soft or "graphitic" form is utilized as a high-temperature lubricant in an oxidizing atmosphere. A particular application for the lubricant is on or in flexible, ceramic-fiber side seals on a continuous glass coating apparatus and the moving edges of glass itself, thereby minimizing any flow to or from the reactor of gaseous reactants.
REFERENCES:
patent: Re31883 (1985-05-01), Bovenkerk et al.
patent: 4146657 (1979-03-01), Gordon
patent: 4206252 (1980-06-01), Gordon
patent: 4264350 (1981-04-01), Thomas
patent: 4271212 (1981-06-01), Stengle
patent: 4285168 (1981-08-01), Scheetz
patent: 4377613 (1983-03-01), Gordon
patent: 4390562 (1983-06-01), Yanagisawa
patent: 4592307 (1986-06-01), Jolly
patent: 4612217 (1986-09-01), Gordon
patent: 4680218 (1987-07-01), Kimura et al.
patent: 4713186 (1987-12-01), Kristen et al.
LandOfFree
Sealing oxidizing atmosphere at high temperatures does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Sealing oxidizing atmosphere at high temperatures, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Sealing oxidizing atmosphere at high temperatures will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-903699