ABSTRACT:
Improved halogenated butyl rubbers are prepared by isomerizing the polymers so that a significant mole fraction of the halogen is in the primary allylic position. The isomerization is carried out utilizing as a catalyst either a Friedel Crafts catalyst or HBr.
REFERENCES:
patent: 2809372 (1957-10-01), Frederick et al.
patent: 3042662 (1962-07-01), Cottle et al.
patent: 3515687 (1970-06-01), Listner
patent: 4486575 (1984-12-01), Newman et al.
patent: 4563506 (1986-01-01), Kowalski et al.
Baldwin Francis P.
Fusco James V.
Gardner Irwin J.
Exxon Research & Engineering Co.
Lipman Bernard
Schofer Joseph L.
LandOfFree
Process for preparing improved halogenated butyl rubbers does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for preparing improved halogenated butyl rubbers, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for preparing improved halogenated butyl rubbers will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-684545