ABSTRACT:
Disclosed are a method and apparatus for improving the fatigue characteristics of a glass optical waveguide fiber. After the fiber is drawn and before it is provided with a protective coating it is heated to a temperature within the annealing temperature range. A filtered gas may be flowed over the fiber during the step of heating.
REFERENCES:
patent: 1438428 (1922-12-01), Dhe
patent: 3589878 (1971-06-01), Achener
patent: 3782914 (1974-01-01), DeLuca et al.
patent: 3788827 (1974-01-01), DeLuca
patent: 3881945 (1975-05-01), Trojer et al.
patent: 4199336 (1980-04-01), Rittler
patent: 4249925 (1981-02-01), Kawashima et al.
patent: 4304582 (1981-12-01), Aussenegg et al.
patent: 4309201 (1982-01-01), Klop et al.
R. Hiskes, "Improved Fatigue Resistance of . . . Optical Fibers" Tech. Digest Conf. on Optical Fiber Communication, Mar. 1979, Washington, D.C.
Bailey Alan C.
Maurer Robert D.
Corning Glass Works
Fisher Richard V.
Simmons, Jr. W. J.
LandOfFree
Method of improving fatigue resistance of optical fibers does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of improving fatigue resistance of optical fibers, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of improving fatigue resistance of optical fibers will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-482196