Process for increasing polyamide molecular weight with organopho

Synthetic resins or natural rubbers -- part of the class 520 ser – Synthetic resins – Mixing of two or more solid polymers; mixing of solid...

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

524 99, 524124, 524606, 524419, C08G 6948

Patent

active

051420007

ABSTRACT:
A process for increasing the molecular weight of a polyamide in the presence of alumina-containing titanium dioxide, said process comprising heating a polyamide containing terminal carboxy and amino groups, and alumina-containing titanium dioxide, in the presence of a catalytically effective quantity of at least one phosphonic acid catalyst and/or ester thereof selected from:

REFERENCES:
patent: 4912175 (1990-03-01), Wheland et al.
patent: 4966949 (1990-10-01), Wheland

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for increasing polyamide molecular weight with organopho does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for increasing polyamide molecular weight with organopho, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for increasing polyamide molecular weight with organopho will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-385704

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.