ABSTRACT:

BACKGROUND OF THE INVENTION
The present invention provides a molding composition of siloxane which is capable of extending mold lifetime that can be realized by adding alkene or acetylene polymerization inhibitors into molds composed of siloxane and are especially indicated in this invention.
The process of making molds (caves) by using solidificable composition of siloxane is primarily done by pouring the composition around objects which will be released and removed after the composition of siloxane solidify, then followed by emptying the caves where the objects were placed before are formed. The glassy or solid molded products will be obtained after the molded material, such as a liquid or resin with a solidifying agent, is added into the caves. The molded material most often used is a polymerizable liquid such as a polyester-styrene resin (unsaturated polyester resin) which will polymerize and solidify after it is injected into the mold caves composed of siloxane. However, since this process (especially for the alkene resin) is exothermic (sometimes highly exothermic reaction), the molds will be damaged after it is reused.
Damage to the molds may occur for several reasons. Some of the more common ways in which the molds are damage occurs where:
1. A part of a solidified composition of siloxane molds adhere to the molded material. The molds composed of siloxane are damaged by the pulling when the molded material is taken out. This is especially true for molds containing juts or fine stripes.
2. The contacting surface of molds composed of solidified siloxane hardens after being reused several times. The molds are ripped and spoiled because the surface lacks softness and elasticity.
Chemical analysis of damaged molds provides the basic explanation for the damage, that is, both of the mixture components such as a polyester resin and styrene, which is usually used as the molding resin to siloxane molds, can permeate into the siloxane molds. Meanwhile, the solidifying catalyst used in unsaturated polyester resins can also permeate into the siloxane molds, which therefore causes polymerization of polymerizable subjects entering into the siloxane molds and generating a crossing net of polystyrene and organic polysiloxane to harden mold surfaces.
To improve and modify the disadvantages of molds composed of siloxane aforementioned, the subject invention the composition of siloxane molds to extend the lifetime by means of dedications in work, professional knowledge, and experiences in design and manufacture.
DESCRIPTION OF THE PRIOR ART
Various types of organopolysiloxanes and silicone compositions have been provided in prior art. For example, U.S. Pat. No. 5,977,249 to Kovar et al., and U.S. Pat. No. 5,196,477 to Arai et al. are illustrative of such prior art. While these units may be suitable for the particular purpose to which they address, they would not be suitable for the purposes of the present invention as heretofore described.
The Kovar Patent relates to compositions which cross link to provide elastomers or polymers with elastic properties. The compositions are transparent and possess a low compression set. The disclosure describes a silicone rubber composition comprising a polyorganosiloxane with at least two alkenyl groups per molecule and a polyorganosiloxane with at least two silicone-bonded hydrogen atoms, an organic sulfur component, and a metallic catalyst.
The Arai Patent discloses a silicone composition comprising a vinyl end-capped polydiogranosiloxane, a linear organohydrogenpolysiloxane having at least two Si—H groups, sulfides and fillers. The organopolysiloxane composition is adapted for use as insulating materials for electric and electronic parts in order to prevent contact failure.
The above mentioned compositions have the disadvantage that they do not provide the compositions which are capable of extending the lifetime of molds composed of siloxane.
SUMMARY OF THE INVENTION
The main object of this invention is to provide the molding composition of siloxane which is capable of extending mold lifetime where inhibitors alkene or acetylene polymerization are mixed in the molds composed of siloxane. The inhibitors can effectively inhibit the release of alkene or acetylene when a resin containing an alkene or acetylene is poured into the molds. This method extends the lifetime of molds composed of siloxane. The inhibitors are compounds primarily containing sulfur, wherein sulfur is the most effective.


REFERENCES:
patent: 5196477 (1993-03-01), Arai et al.
patent: 5977249 (1999-11-01), Kovar et al.
patent: 6010646 (2000-01-01), Schleifstein

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Molding composition of siloxane capable of extending mold... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Molding composition of siloxane capable of extending mold..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Molding composition of siloxane capable of extending mold... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3109648

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.